According to taulman, they recommend a long retract to help with oozing, so I was just going with their recommended numbers. Even with that amount I still get some oozing, so I'm going to try lowering my temp like Scott has recommended. I've been drying the nylon filament in an old toaster oven at 100 degrees, which has helped a lot too.
I've installed Kisslicer, but haven't used it for any prints yet, as I'm not as familiar with how the settings work. Specifically I'm not sure where I compensate for my bed height, as my garolite is over 6mm thick, and I need a +3.4mm offset to avoid crashing the nozzle into the bed. I'm also not 100% on how to fine tune the extrusion volume. Scott, I'm curious why you're using a 3.35mm value for your filament. Is yours actually that diameter, or are you doing that to effectively reduce the volume of material extruded? Mine averages to 3.05mm.