What is governing thickness for PWHT is it weldmetal being welded or thicker component being welded?

ASME B31.3

331.1.3 Governing Thickness. When components are joined by welding, the thickness to be used in applying the heat treatment provisions of Table 331.1.1 shall be that of the thicker component measured at the joint.

Q-1 : If  i have one joint dissimilar butt joint between P1 # 20mm thk and 45mm thk and weld metal thickness is 20mm (40mm portion is made tapper).
Still i hve to do PWHT for this joints as per 45mm.??

(i know as per B31.3 if preheat is applied 95C pwht not req,but what in case of service requirement is PWHT.)

ASME B31.1

132.4.1 The term nominal thickness as used in
Table 132 and Notes is the lesser thickness of (A) or (B)
as follows:
(A) the thickness of the weld
(B) the thicker of the materials being joined at the
weld

Same things applicable as per B31.1 ??


george....@gr.bureauveritas.com

unread,
Sep 22, 2015, 6:24:36 AM9/22/15
to material...@googlegroups.com

For one more time I recommend to read all the relevant chapter of the Code and not isolated paragraphs.
So I would like to draw your attention also to the following paragraphs
132.1.2
132.2 (B)
and to 132.4.2

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Karunakaran Karan

unread,
Sep 22, 2015, 10:26:31 AM9/22/15
to material...@googlegroups.com
Dear Gents,
What is the minimum thickness for PWHT in revision 2014.
Pl.guide me.
Thank you
karunakaran

On 9/22/15, george....@gr.bureauveritas.com
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-weld...@googlegroups.com.
> To post to this group, send email to material...@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/OFE830CE67.C6D3555F-ONC2257EC8.002E0971-C2257EC8.002E85C5%40LocalDomain.
> For more options, visit https://groups.google.com/d/optout.
>


--
*S.KARUNAKARAN*
karu...@gmail.com

george....@gr.bureauveritas.com

unread,
Sep 22, 2015, 11:45:57 AM9/22/15
to Karunakaran Karan

What is the jointed materials Pnos?

Sent from my BlackBerry 10 smartphone.
  Original Message  
From: Karunakaran Karan
Sent: Τρίτη, 22 Σεπτεμβρίου 2015 - 17:26
To: material...@googlegroups.com
Reply To: material...@googlegroups.com
Subject: Re: [MW:23504] Governing Thickness for PWHT(B31.1&31.3)

For more options, visit https://groups.google.com/d/optout.

Hafiz Ali Alvi

unread,
Sep 22, 2015, 11:18:07 PM9/22/15
to material...@googlegroups.com
Q-1 yes PWHT is applicable for joint between 45mm and 20mm. See interpretation of B31.3 

Sent from my iPhone
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

Karunakaran Karan

unread,
Sep 23, 2015, 5:25:57 AM9/23/15
to material...@googlegroups.com

george....@gr.bureauveritas.com

unread,
Sep 23, 2015, 1:31:33 PM9/23/15
to material...@googlegroups.com

I case the applicable Code Section is B31.1:
No PWHT if T as defined in 132.4.1 is < 19.00 mm
No PWHT if T as defined in  132.4.1 is < 25.00 mm and preheat of 95 degC min is applied
No PWHT if T as define in 132.4.1 is between 19 mm and 38 mm (Included) and CE < 0,50 and min preheat 121 degC and max deposited thickness per pass 6 mm



 
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Karunakaran Karan ---23/09/2015 12:26:02---Hello,        P1 GI to P1GI AND PIG1 TO PIG2Karunakaran Karan ---23/09/2015 12:26:02---Hello,        P1 GI to P1GI AND PIG1 TO PIG2


>


--
*S.KARUNAKARAN*
 karu...@gmail.com


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at

george....@gr.bureauveritas.com

unread,
Sep 23, 2015, 1:31:33 PM9/23/15
to material...@googlegroups.com

In case the applicable Code Section is B31.3
No PWHT for all thickness below or equal to 20 mm (2006 edition)


best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Karunakaran Karan ---23/09/2015 12:26:02---Hello,        P1 GI to P1GI AND PIG1 TO PIG2Karunakaran Karan ---23/09/2015 12:26:02---Hello,        P1 GI to P1GI AND PIG1 TO PIG2

From: Karunakaran Karan <karu...@gmail.com>
To: material...@googlegroups.com
Date: 23/09/2015 12:26
Subject: Re: [MW:23512] Governing Thickness for PWHT(B31.1&31.3)
Sent by: material...@googlegroups.com






>


--
*S.KARUNAKARAN*
 karu...@gmail.com


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at

Reply all
Reply to author
Forward
0 new messages