The best results for stainless steels and high nickel alloys are obtained when they are purged to oxygen levels of less than 1%. Purging with four to ten times the required volume is needed to obtain the relatively inert atmosphere. Where uncer- tainty exists regarding the adequacy of the purge, a mine safety oxygen analyzer can be used to check the oxygen level in the purge gas being exhausted from the weld area.
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To unsubscribe, reply using "remove me" as the subject.
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to
materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
To unsubscribe, reply using "remove me" as the subject.
*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."
| Yadav Shiva <luvsh...@gmail.com>
Sent by: material...@googlegroups.com 15-04-2010 07:54
|
|
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To unsubscribe, reply using "remove me" as the subject.
|
dear all according to API 582 CLAUSE 7.3 see the following
"Back purging is required for the GTAW and GMAW processes for welding materials having a nominal chromium content greater than 2l/4% unless the joint is ground or back gouged to sound metal."
the cause is
"back purging gas is selected to prevent oxidation or scale formation on the underside of the weld" --- On Mon, 4/19/10, kannayeram gnanapandithan <kgpan...@gmail.com> wrote: |