Dear All,
I have situation where Air Receiver Vessel made of SS 316 designed as per ASME SEC VIII DIV 1 U stamped shipped to site but not yet installed. The vessel is stored on warehouse in packed condition.
The Present design temperature is 70°C which need to be changed to 85°C.
Can you please suggest which are steps we have to take ? Any code reference for recertification ?
Regards
Praphulla
| From: Praphulla Phirke Sent: Παρασκευή, 23 Οκτωβρίου 2015 - 11:11 To: Materials-Welding Reply To: material...@googlegroups.com Subject: [MW:23779] Vessel Design Temperature Change |
Design only need to be verified, Nothing to do with vessel, However change in temperature is small and only in plus side. Hopefully there will be no R-Stamp.
Thanks & Regards,
Mohd. Azam--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXRHHMQDty7yRzwT%3DUyac6cejjVH5FHHj%3DwaVMEXchd8Ew%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF0493CB18.83F8C0F7-ONC1257EE7.002ED059-1445589080487%40LocalDomain.
This has to be confirm from designer end. Design verification is to be done and confirm from his end that there is no need for any change in vessel Drawing.
Thanks & Regards,
Mohd. Azam
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/005D443A-605C-46D2-964D-E617E589896B%40gmail.com.
| From: Mohd Azam Sent: Σάββατο, 24 Οκτωβρίου 2015 - 08:17 Reply To: material...@googlegroups.com Subject: Re: [MW:23787] Vessel Design Temperature Change |
| From: Praphulla Phirke Sent: Σάββατο, 24 Οκτωβρίου 2015 - 10:38 |
Reply To: material...@googlegroups.com |
Subject: Re: [MW:23795] Vessel Design Temperature Change |
Hi
Please revise the design documents and get it approved by ASME AI & by Client as well.
If already applied for NBR, revise and resubmit for registration again (including the changes).
Regards
P
Govindan
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF626850A7.3C2D53AF-ONC1257EE8.002DBDFB-1445674777932%40LocalDomain.
| From: Perumal Govindan Sent: Σάββατο, 24 Οκτωβρίου 2015 - 11:37 |
Reply To: material...@googlegroups.com |
Subject: Re: [MW:23800] Vessel Design Temperature Change |
Hi Praphulla
The vessel should be rerated. You may use the approach as recommended by NBIC or API-510.
Thanks.
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Hamilton, Ontario, Canada
ca.linkedin.com/pub/pradip-goswami/5/985/299
From:
material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of george....@gr.bureauveritas.com
Sent: Saturday, October 24, 2015
6:32 AM
To: Perumal Govindan;
material...@googlegroups.com
Subject: Re: [MW:23802] Vessel
Design Temperature Change
A Code vessel can not be stamped two times with a Code stamp. In case of repair, alteration or re rating it has to be stamped with the "R" stamp.
Sent from my BlackBerry 10 smartphone.
|
From: Perumal Govindan Sent: Σάββατο, 24 Οκτωβρίου 2015 - 11:37 Reply To: material...@googlegroups.com Subject: Re: [MW:23800] Vessel Design Temperature Change |
Hi
Please revise the design documents and get it approved by ASME AI & by Client as well. If already applied for NBR, revise and resubmit for registration again (including the changes).
Regards
P.Govindan