Dear Experts,
I am pleased to draw your attention and please provide your valuable input / advice / comment / clarification regarding my interpretation as below.
The following is the requirement as referring to the attached 6600028289 (OOK) schedule Q_quality requirements attachment 1 clause 2.2.1.
Quote starts
Quote Ends“ When performing, reviewing or ensuring Nondestructive Testing in VT, MT, PT, RT or UT, he shall be certified in the specific method(s). When performing, reviewing or ensuring Radiographic Testing Film Interpretation (), Inspector shall be certified in ASNT Level II."
My interpretation is RT report shall be reviewed or ensured by the inspector with ASNT Level II certified in RTFI.
And after reviewing or ensuring the reports as per the requirements that report shall endorsed (singed) by that inspector who is qualified in RTFI .
But the vendor is dis agreeing with the my statement.
Please advise me.
Thanks and best regards,
Mohammed Ismail,
Mechanical Inspector,
vendor inspection department,
Velosi.
Dear Sir,
You are correct and just for curiosity what is your vendors interpretation for that paragraph.
Regards,
Hareesh K V
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5525e7c3.e26e440a.3a8a.2d95%40mx.google.com.
Dear Sir,
You are correct and just for curiosity what is your vendors interpretation for that paragraph.
Regards,
Hareesh K V
On Apr 9, 2015 8:28 AM, "Lakshman" <lakshma...@gmail.com> wrote:
Hi friend, you are correct, but let us understand why client is not accepting and what is his views?
We should know theirs interpretation also prior to confirm...![]()
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAVxyZJcSoB1Q%2BwyGKz7c19hf8CS872ruAy8pXCr5vSmzw%40mail.gmail.com.
Mohammed Ismail
Inspection Engineer-Mechanical
Phone : +966 38394292 Ext - 243
Mobile + 966 565 063 994
Fax : + 966 3 8393671
Velosi Saudi Arabia
Dammam-KSA.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWuSzEttudxDmfd38WGKaKMXop%3DkpUTM-RFDMwVFJGqq255Rg%40mail.gmail.com.
Dear sir,
Please share with the vendor the guidelines of ASNT about level 2 in RT and RTFI.
RT qualification from ASNT Level 2 is an operator level qualification. In INDIA, an ASNT level 2 person cannot operate a radiography camera as we have to follow the regulations of AERB .Outside INDIA an ASNT level 2 person can operate a radiography camera.
In ASNT level 2 in RT there is nothing regarding the evaluation of radiography film.
An ASNT RTFI level 2 person is qualified to evaluate Radiography film, interpret it and is qualified to sign the report.
It is a general perception that an ASNT Level 2 in RT is qualified for film interpretation and that is wrong.
Best regards,
Hareesh K V
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF2Z%3DtWUy2238E%3DH9Qjee4fj5gszGVbDcB01a%3D%2BpOyPC7nSZuA%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAUuVqzEDmm%2BfeE%3DM%2BFY4KtM1CtmJ3Y-Hp%3DavwQy%3DKrroA%40mail.gmail.com.