Dear experts,
I have to weld one plate which is on the top of shell plate which is fillet joint,
Which welding position we have to choose 4 G or 4 F, 
2nd it is not completely 4F,  it is like 3 F.

your quick response will be highly appreciated.

Regards
aslam

VISHNUDAS MAVUNKASHERY

ongelezen,
15 feb 2017, 05:19:1315-02-2017
aan material...@googlegroups.com
attaching a photo of joint will b appreciated


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA68Awkw8NL%2BacUp547wN4vPtBKuOr%2B18dmeVYD0zpBEfPWT7A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
VISHNUDAS MURALI MAVUNKASHERY

Umar Daraz Khan

ongelezen,
17 feb 2017, 21:45:3517-02-2017
aan material...@googlegroups.com
Dear
I have attached the photos showing position of joint
Regards
Umar Daraz Khan

IMG_20170217_110523587.jpg
IMG_20170217_110544851.jpg
IMG_20170217_110559818.jpg

Prasad Rode

ongelezen,
19 feb 2017, 23:40:1819-02-2017
aan Materials & Welding
It seems to he 4F.

ECHARU

ongelezen,
20 feb 2017, 22:09:5820-02-2017
aan material...@googlegroups.com
Friend 3F vertical, 4F overhead, why u have don't choose it.

From: Prasad Rode
Sent: ‎20-‎02-‎2017 07:40
To: Materials & Welding
Subject: Re: [MW:26108] welding positionpp

It seems to he 4F.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9acb4b6-9d9b-4712-86d4-b548119e5b0a%40googlegroups.com.

Gopi Krishna Banerjee

ongelezen,
21 feb 2017, 00:10:2021-02-2017
aan material...@googlegroups.com
Please qualified welder in both position , 3F & 4F Position (  if Welder Qualified in 3G & 4G Position welder  will be  eligible for  3F & 4F Position welding  as per ASME Sec. IX. ).

On Mon, Feb 20, 2017 at 8:24 PM, ECHARU <usa...@gmail.com> wrote:
Friend 3F vertical, 4F overhead, why u have don't choose it.

From: Prasad Rode
Sent: ‎20-‎02-‎2017 07:40
To: Materials & Welding
Subject: Re: [MW:26108] welding positionpp

It seems to he 4F.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/58ab0322.49b3df0a.1fa4e.ff01%40mx.google.com.

George Dilintas

ongelezen,
22 feb 2017, 22:39:2322-02-2017
aan Meghanadh K
It seems 4F to me


For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Allen beantwoorden
Auteur beantwoorden
Doorsturen
0 nieuwe berichten