Preheat decrease >50deg.C

86 views
Skip to first unread message

Vadivel Mahadevan

unread,
Apr 21, 2017, 8:13:29 AM4/21/17
to Materials & Welding
Dear Experts,
I have a doubt.
In ASME sec. IX,in many Welding process it is mentioned as "Preheat decrease >55 deg. C"
can you let know what it means exactly.. How to intrepret this variable..
Thanks in advance
Vadivel M

Kannayeram Gnanapandithan

unread,
Apr 22, 2017, 2:07:19 AM4/22/17
to materials-welding
In PQR, if ur preheat temp is 100,℃, in wps u can mention minimum 45℃, ( 100-55=45,) if it is mentioned less 45, requalification required

On 21-Apr-2017 5:44 PM, "Vadivel Mahadevan" <vadivel...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (vadivel...@gmail.com) Add cleanup rule | More info
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cf10576a-f335-4b14-923d-75e98c1e3165%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Prakash Hegde

unread,
Apr 22, 2017, 10:15:22 AM4/22/17
to kgpan...@gmail.com, materials-welding
Just to add to Mr Mahadevans reply 
You req to preheat Even the thk of the job is very less(provided you use the same wps n spporting pqr) thete is no restriction on higher side preheat temp.
Regards
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOM%2BgH%3DVPSunTQoqMp7SiLsk_X_xpsVo4D3eZvuZJB7-Q%40mail.gmail.com.

Vadivel Mahadevan

unread,
Apr 23, 2017, 2:01:05 AM4/23/17
to Materials & Welding
Thank you gentlemen..
With regards
Vadivel M