Hi friends,
We have a big pipe line job in water segment.
We are planning to implement FCAW or GMAW technique to expedite the welding activity…
Please suggest me that which technique is most favorable for IS2062 material (equivalent to Pno 1) at site for 5G or 6G position…..
Your detail explanation will be more helpful on selecting the process….
Also in terms of cost – which will be economical for the project ….
Thanks & Regards,
Lakshman Kumar B,
Project Manager.
Navayuga Engineering Company LTD
Corp Off: Plot no 379, Road No 10,
Jubileehills, Hyderabad.500033 India.
Tel - +91 -40-2333 9990/91/92 – Ext 398
Fax: +91-40-2333 7789
Mob - +91 9440031459.
Email –lakshma...@navayuga.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003601d22f41%241a710580%244f531080%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
<image001.jpg>

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePw3gXNgxXZntjZ_wkY5Z4yiAvZvUOHb4YQbRSBnktNWQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/lmujqb6xnnfgcx2bm8cj7vh3.1477462999974%40email.android.com.
Hi Mr. Neilash Kumar,
It is 120 Inch (3000Mm Dia) with 20 mm thick for a water transmission project.
Thanks & Regards,
Lakshman Kumar B,
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4184246A-BDD1-44E7-90A0-D1ADB44AD891%40yahoo.com.
Hi friends,
We have a big pipe line job in water segment.
We are planning to implement FCAW or GMAW technique to expedite the welding activity…
Please suggest me that which technique is most favorable for IS2062 material (equivalent to Pno 1) at site for 5G or 6G position…..
Your detail explanation will be more helpful on selecting the process….
Also in terms of cost – which will be economical for the project ….
Thanks & Regards,
Lakshman Kumar B,
Project Manager.
Navayuga Engineering Company LTD
Corp Off: Plot no 379, Road No 10,
Jubileehills, Hyderabad.500033 India.
Tel - +91 -40-2333 9990/91/92 – Ext 398
Fax: +91-40-2333 7789
Mob - +91 9440031459.
Email –lakshma...@navayuga.com
Alan Denney
AKD Materials Consulting Ltd
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of dilintas
Sent: 26 October 2016 07:23
To: material...@googlegroups.com
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003601d22f41%241a710580%244f531080%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePw3gXNgxXZntjZ_wkY5Z4yiAvZvUOHb4YQbRSBnktNWQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/lmujqb6xnnfgcx2bm8cj7vh3.1477462999974%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
Hi Lakhsman,
Both the processes are popular choices for pipeline welding. Mechanization is the key. In general controlled surface transfer process e.g. STT or RMD are very conveniently used for long pipeline welding projects to cut down the production time and defect rates.
The attached documents provide some insights to such projects. Use the info at your discretion.
Thanks.
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist ,
ca.linkedin.com/pub/pradip-goswami/5/985/299
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAALpHkqFntblOtVlMJ77H09YBAAAAAA%3D%3D%40quickclic.net.
<Mechanized-Pipeline-Welding-Magnatec.pdf>
![]()
This message is eligible for Automatic Cleanup! (materials-welding@googlegroups.com) Add cleanup rule | More info
Dear Lakshman,Good morning, as told by Pradip sir it's has to be root weld by GMAW-STT, followed by SAW -Machine Welding column and boom with roller bed both in site or shop.Since 3meter OD little bit difficult with Mechanisation process, and I have practical experience with Magna tech and lone star machine up to 48 inch only.I don't see any external band for 3meter OD.Even in machine welding in order to increase productivity you can choose Twin wire SAW process.Further any clarification let me know to clarify.
Hi Lakhsman,
Both the processes are popular choices for pipeline welding. Mechanization is the key. In general controlled surface transfer process e.g. STT or RMD are very conveniently used for long pipeline welding projects to cut down the production time and defect rates.
The attached documents provide some insights to such projects. Use the info at your discretion.
Thanks.
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist ,ca.linkedin.com/pub/pradip-goswami/5/985/299
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003601d22f41%241a710580%244f531080%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4184246A-BDD1-44E7-90A0-D1ADB44AD891%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/008401d22fb6%245faad430%241f007c90%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAALpHkqFntblOtVlMJ77H09YBAAAAAA%3D%3D%40quickclic.net.
<Mechanized-Pipeline-Welding-Magnatec.pdf>
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0FD338FD-704C-442D-9BF4-6058762CE43D%40yahoo.com.
Dear Mr. Pradip And all friends…
Thanks a lot for sharing your valuable inputs, and really it’s a great learning and good understanding also….
Further I would like to bring to your notice for the following key parameters…
(please see the images also and pls be informed that it is of water pipe line and cant able to correlate with Oil & Gas Cross country pipe lines) the following limitations we have …
1. Pipe are not in exact round shape and most of the time pipes internal will be supported by spider pipes (bracings) to retain its shape, however those will be removed during execution time. Here 120 Inch dia (3000Mtr dia) with a thickness of 16/18 mm – D/T is almost 190…
Hence internal / external fitup clamps are not possible.
Edge preparation at site is not feasible, and we have a limitation to restrict to factory made bevel or bevel preparation by free hand ( not that much accurate)
2. Pipe will be laid in the trench one after one – (like as O&G it is not welded outside the trench and lowering the pipe line with side booms) – after completing one pipe welding another pipe will be laid and will continue further…
3. Hence pipe are directly laying in the trench, we didn’t have much clearance under the pipe
Hence big weld heads are not possible to use.
We can’t able to go for full automation like as CRC Evans and all (earlier I worked in Reliance and in CRC welding)
4. Like as O&G – alignments are not too much straight, and didn’t have free ROU clearances –
O&G lines has to laid far from villages and dense areas, where as Water lines have to laid near to villages and cities by connecting all the areas.
Like as in O&G or for full automation – we can’t provide the clear work front.
Water lines have the above limitations and so only we should be particular about the process…
Any way I understood Any of the process can be implemented.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAALpHkqFntblOtVlMJ77H09YBAAAAAA%3D%3D%40quickclic.net.
The issue of using IS 2062 plate for the pipes as has being enquired rihghty so by mr. Nautiyal remains unanswered. Can we get an idea about it?
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/00bd01d2302a%248c645130%24a52cf390%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------
Sir
It is possible that if you use Pulsed MIG for Root Run only and Subsequent Run by FCAW Process for this Projects.
G. K. Banerjee.
NAGPUR.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003601d22f41%241a710580%244f531080%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4184246A-BDD1-44E7-90A0-D1ADB44AD891%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/008401d22fb6%245faad430%241f007c90%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAALpHkqFntblOtVlMJ77H09YBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/00bd01d2302a%248c645130%24a52cf390%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1fd5667b6644a788fa366c75d04e5dd%40MUMEXG02.TCE.COM.