EXCEL SHEET : WELD CONSUMABLE QUANTITY CALCULATOR

30,286 views
Skip to first unread message

Vikas Bhandari

unread,
Nov 3, 2015, 2:33:15 AM11/3/15
to material...@googlegroups.com
Hi

Can anyone share a standard excel sheet  for pipe butt weld consumable quantity calculation?

Many thanks

Best regards

Vb

waqas suleman

unread,
Nov 4, 2015, 10:47:13 PM11/4/15
to material...@googlegroups.com
Dear Members,

I am also waiting for the same below requested file.

Regards,

Waqas Suleman
Mob. 00966 59 359 0798

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACpSjOn%3DhNb3z324Ci-%3D94bUSjpD7oVQUJBeWVokThmCi0GL%2Bg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Karthik

unread,
Nov 5, 2015, 12:09:05 AM11/5/15
to material...@googlegroups.com
 Hi, 
The attached file might be useful to you
Thanks& Regards,
 
(Karthik)
QA/QC Manager 
CMI-Thai Services Co.,Ltd. 
50/35 Sermsuwan Road,Tambol Maptaphut 
Amphur Muang Rayong,Rayong 21150
Thailand
www.cmi-services.com 
Tel : +66 38 691 390-2 ext.103 
Fax : +66 38 682 338 
Mobile: +66 892512282 
E-mail : karth...@cmi-services.com
               Karth...@yahoo.com



Weld Deposit and Electrode Calculations.zip

MITHLESH

unread,
Nov 2, 2018, 2:41:23 AM11/2/18
to Materials & Welding
HI SIR,
In attached file, ID means inch dia? and another thing is deposition rate of SAW not given. is it not applicable for SAW? 




Karthik

unread,
Nov 2, 2018, 4:28:27 AM11/2/18
to Materials & Welding
Hi,
The attached file might be useful to you.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthi...@yahoo.com



HI SIR,

For more options, visit https://groups.google.com/d/ optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Weld Deposite Calculations.xls

williams p wilson

unread,
Apr 26, 2023, 4:12:38 AM4/26/23
to material...@googlegroups.com
Dear Sir,

Thanks for sharing the file.
It is password protected, do you have the password

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

Bharathi Raja.E

unread,
Jul 3, 2024, 5:19:48 AM7/3/24
to Materials & Welding
  Dear Sir,

Thanks for sharing the file.
It is password protected, do you have the password


Karthik

unread,
Jul 3, 2024, 6:12:27 AM7/3/24
to Materials & Welding
Weld Deposit and Electrode Calculations.zip
Reply all
Reply to author
Forward