Weld and Test Plan

129 views
Skip to first unread message

Shahil Saini

unread,
Feb 9, 2022, 11:31:16 PM2/9/22
to material...@googlegroups.com
Hello everyone,

My question is regarding weld and test plan preparation. In the weld and test plan, 
Q1. How can one select which process is required at the Long seam or Circumferential seam? and
Q2. using which one can prepare weld and test plan GA/Part drawing or by any other way?

Regards
Shahil Saini
(PGET-Welding)

Jenish Mistry

unread,
Feb 10, 2022, 2:33:13 AM2/10/22
to material...@googlegroups.com
Hi,

For Q1 ,Case 1 :  For Selection of Process some Client already mentioned in their approved Drg. for which process you should have to follow.
             Case  2 : If in approved Drg. process is not mentioned than before start of production weld first you should have to approve weld Map from client  which include process (with sequence)                                  with joint configuration ( L/s ,C/S. etc..)

For Q2 ,Test Plan should be as per GA Drg,Part Drg,Client Specification & Client Purchase Order.GA Drg,Part Drg,Client Specification & Client Purchase Order requirement should comply in Test plan.

I hope your doubt is clear now.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-V_pNPmg%2BqZz8oD_iLjqA_o-Ci6Vs3Wqx8iWjQTLFyRA%40mail.gmail.com.


--
Thanks for your best support.

Regards,
Jenish Mistry

Shahil Saini

unread,
Feb 10, 2022, 3:47:05 AM2/10/22
to jenishmi...@gmail.com, material...@googlegroups.com
Hello jenish sir,

From where i begin for weld & test plan preparation, Is there any sequence to follow for the preparation of the weld & test plan.

Kindly advise further,

Thanks & Regards
Shahil Saini
(PGET-Welding)

Ron Mays

unread,
Feb 10, 2022, 10:16:17 PM2/10/22
to material...@googlegroups.com
Jenish, each of the items listed in the attached list needs to be "signed off" when completed.
Hope this helps.

Ron Mays

Suggested Items for ITP.DOC

Shahil Saini

unread,
Feb 10, 2022, 10:50:16 PM2/10/22
to ronma...@gmail.com, jenishmi...@gmail.com, material...@googlegroups.com
Hello Ron,

Is this attached list is related to the weld & test plan?

Regards
Shahil Saini 
PGET- Welding

Ron Mays

unread,
Feb 11, 2022, 12:15:05 AM2/11/22
to Shahil Saini, jenishmi...@gmail.com, material...@googlegroups.com
Yes, that is correct. 
Ron Mays

Ron Mays Welding Advice
ABN 59573532422
8 Ronald Avenue
Selby 3159
0417 354 108 mob.
ronma...@gmail.com



Shahil Saini

unread,
Feb 16, 2022, 11:36:04 PM2/16/22
to Jenish Mistry, material...@googlegroups.com
hello jenish,

I have all the material mentioned by you in the above email, after this from where to begin the preparation of weld and test plan and how to use the above mentioned material parallely??

Regards
Shahil Saini
PGET-Welding

On Thu, Feb 10, 2022 at 3:17 PM Jenish Mistry <jenishmi...@gmail.com> wrote:
Hey,

Up to my experience ,Basic methodology for preparation of Weld Test plan is as follows.

PO--->Customer Specification with Design data ( for understand equipment Service requirement)----> Approved drawing ---->Approved ITP/QAP & Procedure

I think if you follow above sequence than you may get clear idea about test plan.
Regards,
Jenish Mistry
09033476117
Reply all
Reply to author
Forward
0 new messages