Dear Sir

Please support us for below concern:

i carried out PQR with GTAW & SMAW (No Impact, GTAW deposit weld is 5 mm & SMAW deposit weld is 42.64 mm), the test coupon is 23.82mm so the qualified thickness range will be 5 to 47.64 mm.

If i want to make new WPS based on the above PQR (GTAW WPS), is it permissible to put qualified thickness range to be 1.5 to 10 mm based on GTAW deposit weld (5mm)?
Please support with evidence 

 

Regards


George Dilintas

ongelezen,
16 jan 2017, 10:45:5616-01-2017
aan Meghanadh K
You have to take into account that in ASME IX the base metal thickness is quit different from deposited thickness.
So the base metal thickness, based on that PQR, is determined my the 23,82 mm.
So your base metal thickness approval range (no impact) would be the same as previously

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1700757652.238572.1484052246572%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Allen beantwoorden
Auteur beantwoorden
Doorsturen
0 nieuwe berichten