Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

harenath jha

belum dibaca,
15 Apr 2020, 02.28.5415/04/20
kepadamaterial...@googlegroups.com
What is the conditions of material.
Is it heat treated normalised or something else.

On Wed, Apr 15, 2020, 10:31 Chiranjeevi A <chiranjee...@gmail.com> wrote:
Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xJKPZj%2Bf35s8imSXNUXKDy%3DEKgyqDtZadtu62dHMgHmw%40mail.gmail.com.

Perumal Govindan

belum dibaca,
15 Apr 2020, 02.28.5515/04/20
kepadamaterial...@googlegroups.com

Please check for your project Piping/Welding Specification/standards/fabrication procedure of inconel Piping.
If not found, check with manufacturer recommendation and get it approved by client.

On Apr 15, 2020 10:30 AM, "Chiranjeevi A" <chiranjee...@gmail.com> wrote:
Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Chiranjeevi A

belum dibaca,
15 Apr 2020, 03.26.2515/04/20
kepadamaterial...@googlegroups.com
Dear Harenath,

       Due to improper storage, the thermowell of Inconel 601 got corroded. For these items can we do pickling and passivation? 

SAMEER LANDGE

belum dibaca,
15 Apr 2020, 06.57.3415/04/20
kepadamaterial...@googlegroups.com
ASTM A380 is a good ref.  It give a list of possible solutions to use and some basic guides. 

Regards 
Sameer 

Sent from my Huawei phone

harenath jha

belum dibaca,
15 Apr 2020, 06.57.3415/04/20
kepadamaterial...@googlegroups.com
Again... Please what is the as shipped condition... If it is not heat treated then u can not do passivation. If it is heat treated then passivation can be done Please refer astm a 380 for more details...  Still you are in doubt please let me know..

james gerald

belum dibaca,
15 Apr 2020, 07.23.1915/04/20
kepadamaterial...@googlegroups.com
I suppose there are 2 types of Nickel Alloys, Solid solution strengthened and Precipitation Hardened alloys.

Inconel 601 falls under Solid solution strengthened and supplied in  Solution Annealed Heat Treated condition.

ASTM A 380 is pickling and passivation standard for stainless steel.

it is better to contact the Manufacturer regarding Pickling and passivation to remove corrosion deposits.

Thanks & Regards

J.Gerald Jayakumar




Perumal Govindan

belum dibaca,
15 Apr 2020, 07.30.5915/04/20
kepadamaterial...@googlegroups.com

Please refer packing, transportation and preservation procedure of the manufacturer.

That might contains the preservation details otherwise better to get advice from the manufacturer.

On Apr 15, 2020 10:30 AM, "Chiranjeevi A" <chiranjee...@gmail.com> wrote:
Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

james gerald

belum dibaca,
15 Apr 2020, 07.59.5015/04/20
kepada'james gerald' via Materials & Welding
Please check attached Article for Pickling of Nickel alloys

Thanks & Regards

J.Gerald Jayakumar




fabricating Nickel Alloys.pdf