This is with reference to Insulating Joint being installed on Steel pipelines to isolate the aboveground section from the underground section. I needed to know what is the advisable position for installing the same? Should IJs be installed aboveground or is it OK if the same is buried below ground? Also our current practise is we provide Cathodic protection to the underground portion and the portion above the IJ is ideally protected by painting. In some cases the portion above the buried IJ is also coated till the point it comes aboveground. Please provide me with suggestion / recommendations regarding the same.
For some IJs we have started exposing the IJs and keeping it exposed in a chamber & filling it with sand. Is this a viable solution? Please advise
Hi,
To the best of my knowledge and my practice that IJ’s are always to be installed just above ground.
Means – where the pipe came out from the UG – after that we have to place the IJ, and IJ is visible and accessible.
Based on the environment, utilized hardware, and situation we may do painting or not…
Thanks & Regards,
Lakshman Kumar B,
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/794e4e3a-263b-4841-afd8-4c6007dd3a3f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Hi,
To the best of my knowledge and my practice that IJ’s are always to be installed just above ground.
Means – where the pipe came out from the UG – after that we have to place the IJ, and IJ is visible and accessible.
Based on the environment, utilized hardware, and situation we may do painting or not…
Thanks & Regards,
Lakshman Kumar B,
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mahanagar Gas
Sent: Tuesday, November 22, 2016 12:02 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25751] Placement of Insulating Joint in pipeline changing medium from soil to air
This is with reference to Insulating Joint being installed on Steel pipelines to isolate the aboveground section from the underground section. I needed to know what is the advisable position for installing the same? Should IJs be installed aboveground or is it OK if the same is buried below ground? Also our current practise is we provide Cathodic protection to the underground portion and the portion above the IJ is ideally protected by painting. In some cases the portion above the buried IJ is also coated till the point it comes aboveground. Please provide me with suggestion / recommendations regarding the same.
For some IJs we have started exposing the IJs and keeping it exposed in a chamber & filling it with sand. Is this a viable solution? Please advise
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/794e4e3a-263b-4841-afd8-4c6007dd3a3f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003601d24495%2496bb0320%24c4310960%24%40gmail.com.
This is with reference to Insulating Joint being installed on Steel pipelines to isolate the aboveground section from the underground section. I needed to know what is the advisable position for installing the same? Should IJs be installed aboveground or is it OK if the same is buried below ground? Also our current practise is we provide Cathodic protection to the underground portion and the portion above the IJ is ideally protected by painting. In some cases the portion above the buried IJ is also coated till the point it comes aboveground. Please provide me with suggestion / recommendations regarding the same.
For some IJs we have started exposing the IJs and keeping it exposed in a chamber & filling it with sand. Is this a viable solution? Please advise
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHwwqE-A6AsQKM3AVOXtDDUgFBUREb9PXtbFMpfsTwKxfLxzzw%40mail.gmail.com.
Hi – pls correct it, it’s not 220 V
it’s hardly 50 V DC
--
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/794e4e3a-263b-4841-afd8-4c6007dd3a3f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHwwqE-A6AsQKM3AVOXtDDUgFBUREb9PXtbFMpfsTwKxfLxzzw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
Best Regards,
Joydev Dalai
Dy. Manager - QA/QC
JHPL Project,
Kalpataru Power Transmission ltd.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFQz-VLGBLKdNNQ2Zq6_EcR04c-BcRGXRtNA9dRBzG4SZdZYqg%40mail.gmail.com.
This is with reference to Insulating Joint being installed on Steel pipelines to isolate the aboveground section from the underground section. I needed to know what is the advisable position for installing the same? Should IJs be installed aboveground or is it OK if the same is buried below ground? Also our current practise is we provide Cathodic protection to the underground portion and the portion above the IJ is ideally protected by painting. In some cases the portion above the buried IJ is also coated till the point it comes aboveground. Please provide me with suggestion / recommendations regarding the same.
For some IJs we have started exposing the IJs and keeping it exposed in a chamber & filling it with sand. Is this a viable solution? Please advise
--