Hi
Also check your Client requirement / data Sheet of fuel oil tank for design metal temperature and you may consider the impact test requirement.
Regards
Govin
Hi
Please consider API 650 only for qualifying WPS/PQR.
Regards
Govin
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b751b08a-e0c5-4b0d-8b76-34555fc91bcd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
| From: SA Sent: Σάββατο, 17 Οκτωβρίου 2015 - 10:57 To: Materials & Welding Reply To: material...@googlegroups.com Subject: [MW:23724] Impact Test Requirement for Welds of API-650 Storage Tank when Design Metal Temperature is below -7°C |
First of all, ASME SEC.IX does not say about requirement/exemption for impact test.
As per QW-170 of ASME SEC.IX, requirement of impact test, acceptance criteria, specimen requirement etc. are in accordinance with other code section that require impact test.
In your case if design code API-650 ask for impact test & if welding procedures to be qualified as per ASME SEC.IX then all procedures should be qualified with impact test considering all essential & supplementary essential variables for each welding process.
--
Design code to be followed for impact test requirements. Follow API 650.
--