Can anybody suggest the consumable brands/mfr name who can give guaranteed results (if possible pl. attach data sheet)  for high temperature Stress Rupture testing of all batches of welding consumables used at 1000°F & 30ksi stress. The time of failure shall exceed 900 hrs.

Thanks in adv.


S.Mohammed

unread,
Aug 26, 2015, 11:48:40 PM8/26/15
to Materials & Welding
Expert opinion needed.

pgoswami

unread,
Aug 27, 2015, 1:49:14 AM8/27/15
to material...@googlegroups.com, Mr Pradip Goswami
Hi,
Your  query  is too general. What's the design code ,design  specifications  and intended applications ? To the best of my knowledge,  these steels  are used  for hydroprocessing equipments. 
Appreciate your response with more details.

Thanks. 

P.Goswami. 


-------- Original message --------
From: "S.Mohammed" <mohd...@gmail.com>
Date: 2015-08-26 20:54 (GMT-07:00)
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:23352] Welding consumables (2.25Cr-1Mo-0.25V) with guaranteed stress rupture strength

Expert opinion needed.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/27b7de07-9427-4e41-92b0-125ff396af62%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

RAJENDRA PRASAD TRIPATHI

unread,
Sep 10, 2015, 8:50:28 AM9/10/15
to Materials & Welding, R.Ba...@ticb.com
D&H Secheron make Cromotherme 2V(MOD).
Technical leaflet is enclosed.
You may be sent further query on following mail ID

Thanks
Vinay Tripathi
Cromotherme-2V(Mod) (1).jpg

Shamal Daw

unread,
Sep 12, 2015, 4:10:00 AM9/12/15
to material...@googlegroups.com
Hi

Do you need SRT according to ASME BPVC VIII div 2

540 deg 210 Mpa for 900 hour
Or

It also depends on the client requirement: Eg :chevron
538deg 207Mpa 1000 hour

Results are different for SRT

Regards

Shyamal das