Dear all
 I am chit ko from Myanmar. i want to know " API 650 RT acceptance Criteria" refer to ASME VIII Division 1?

Raghuram Bathula

ongelezen,
22 jan 2021, 03:51:0222-01-2021
aan Materials-Welding
yes, read para 8.1.5

On Fri, 22 Jan 2021 at 14:17, chitko khaing <chitkokh...@gmail.com> wrote:
Dear all
 I am chit ko from Myanmar. i want to know " API 650 RT acceptance Criteria" refer to ASME VIII Division 1?

--

STEPHEN QM

ongelezen,
22 jan 2021, 23:48:0322-01-2021
aan material...@googlegroups.com
Isn't it 6.1.5 sir?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmko0pKOte0yMLJU5Q9yXqQH-tQORAE5Bki_URiPgCTQw%40mail.gmail.com.

Raghuram Bathula

ongelezen,
22 jan 2021, 23:50:0222-01-2021
aan Materials-Welding
pl. check latest edition (paragraph numbers may vary)

Pankaj Kolhe

ongelezen,
28 mrt 2021, 08:33:3828-03-2021
aan materials-welding
Yes

On Fri, Jan 22, 2021 at 2:17 PM chitko khaing <chitkokh...@gmail.com> wrote:
Dear all
 I am chit ko from Myanmar. i want to know " API 650 RT acceptance Criteria" refer to ASME VIII Division 1?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Tamil

ongelezen,
29 mrt 2021, 06:55:2329-03-2021
aan Materials & Welding

chandrakant mohikar

ongelezen,
29 mrt 2021, 11:50:3829-03-2021
aan material...@googlegroups.com
Ref: API 650: 8.1.5 Radiographic Standards
Welds examined by radiography shall be judged as acceptable or
unacceptable by the standards of Paragraph UW-51(b) in Section
VIII of the ASME Code

On Fri, Jan 22, 2021 at 2:17 PM chitko khaing
<chitkokh...@gmail.com> wrote:
>

Ying Piu Ng

ongelezen,
19 okt 2021, 23:28:0419-10-2021
aan material...@googlegroups.com
Dear Experts,

I am working on the construction of aboveground circular steel water storage tank. The thickness of the shell plate measures 25mm. 

I wonder if there is any limit on the shell plate thickness which requires 2 side welding. Look forward to your kind advice.

Regards
Patrick

Ying Piu Ng

ongelezen,
19 okt 2021, 23:40:5319-10-2021
aan material...@googlegroups.com
As an additional note, I am referring to submerged arc welding for horizontal seams and wonder if there is a limit on the shell plate thickness which requires 2-side welding. 

Patrick

james gerald

ongelezen,
20 okt 2021, 04:46:0320-10-2021
aan material...@googlegroups.com
The welding may be performed using a Single sided Bevel or Double sided bevel and there is no specific requirement in API 650 except that it shall be Full penetration weld (complete penetration and complete fusion). see snap shot below.
Inline image


 Moreover the Welding code specified by API 650 is ASME Sec.iX which do not have any requirement 
for Single sided/double sided  (for WPS/PQR requirement) See snap shot below

Inline image

  See some snap shots of API 650

Inline image
Inline image
 Please also see snap shot for permanent Backing.
Inline image

There are certain advantages and disadvantages without code restriction on using single sided / double sided Joint

1.  For higher thickness using double sided bevel results in Less Welding consumable consumption & cost.
2. incase if you use single sided bevel with Backing then to obtain complete penetration for double sided bevel back grinding/gouging is essential
3. If you use Automatic welding in 2G position then set-up arrangements for both sides are required.

Thanks & Regards

J.Gerald Jayakumar