Reviewing a material test report (MTR) of SA-516-70 certified as per ASME 2010 Ed 2011àddenda and MTR complies with all the requirements. The Job is to be U stamped per ASME 2013 ED. Theres no requirement of materials to be certified to làtest code editions in contractual documents. Since job is to be code stamped per 2013 Ed, should material also be recertified as per ASME 2013 Ed?

george....@gr.bureauveritas.com

unread,
May 7, 2015, 10:25:56 PM5/7/15
to New91
Re-certified no but checked for compliance with applicable edition and addenda yes

Sent from my BlackBerry 10 smartphone.
From: New91
Sent: Πέμπτη, 7 Μαΐου 2015 - 20:07
Subject: [MW:23228] ASME UG-10 interpretation

Reviewing a material test report (MTR) of SA-516-70 certified as per ASME 2010 Ed 2011àddenda and MTR complies with all the requirements. The Job is to be U stamped per ASME 2013 ED. Theres no requirement of materials to be certified to làtest code editions in contractual documents. Since job is to be code stamped per 2013 Ed, should material also be recertified as per ASME 2013 Ed?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ea56d2f0-37bb-467e-b738-5edb4b826c44%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Makrand Sakpal

unread,
May 8, 2015, 4:04:45 AM5/8/15
to material...@googlegroups.com
But suppose in case if material is not complying with latest code edition then what to do? Re-certification?

george....@gr.bureauveritas.com

unread,
May 8, 2015, 6:01:19 AM5/8/15
to material...@googlegroups.com

No, you reject it, unless you can perform tests which will demonstrate compliance with new Code Edition and Addenda.
You can not certify anything which is not in compliance with the Code
This is not the meaning of UG-10.
You can certify a material, using UG-10, which was not tested & certified & identified by the manufacturer in accordance with the Code, but it is complying with the Code. This is the meaning of UG-10
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Makrand Sakpal ---08/05/2015 11:04:46---But suppose in case if material is not complying with latest Makrand Sakpal ---08/05/2015 11:04:46---But suppose in case if material is not complying with latest code edition  then what to do? Re-certi

Dindo

unread,
May 9, 2015, 12:23:52 AM5/9/15
to material...@googlegroups.com
Yes, you can re certify the material, if it is not complying, then what will you do? will you just throw the thing in the waste bin?

You can do it by checking it with with ASME 2013 Edition Sectiion II Part A, Mandatory Appendix II Table II-200-1 (those manufactured to 1988 thru 2010 Edition)

Also, SA516 / SA516M is identical with ASTM Standard A516 / A516M from 1986 thru 2006 with the latest adopted Edition being 2006

So, if it is within these years of manufacture, you can do you certification.

Prakash Gotimukul

unread,
May 12, 2015, 11:56:05 PM5/12/15
to materials-welding
Nothing can be certified or accepted unless it complies with code. 

Rgds
G.Prakash
AIS, AIA LLC TX, USA

Vishnu GK

unread,
Jun 29, 2015, 4:11:36 AM6/29/15
to material...@googlegroups.com
plate astm 516 to sOn Thursday, May 7, 2015 at 9:07:26 PM UTC+4, New91 wrote:
> Reviewing a material test report (MTR) of SA-516-70 certified as per ASME 2010 Ed 2011àddenda and MTR complies with all the requirements. The Job is to be U stamped per ASME 2013 ED. Theres no requirement of materials to be certified to làtest code editions in contractual documents. Since job is to be code stamped per 2013 Ed, should material also be recertified as per ASME 2013 Ed?

I Need to recertify Astm 516 to sa 516.can Anyone provide me a recertification format for this.

Prakash Gotimukul

unread,
Jun 30, 2015, 2:23:27 AM6/30/15
to materials-welding
Code edition applied includes material also. 2013 edition gives details of how to accept material of earlier/later editions of code. Pl refer appendices

Rgds
G.Prakash
AIS, AIA LLC TX, USA

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

John Henning

unread,
Jun 30, 2015, 12:42:40 PM6/30/15
to material...@googlegroups.com

you will not have to recertify the material.  For example, please read Section VIII Division I Nonmandatory Appendix 43 and specifically 43-3-3 (similar instruction for Sc I).  This directs you to ASME Section II-Part A but not very cleanly.  You will need to go to Mandatory Appendix II.  This appendix has a table of all ASME/ASTM specifications and the acceptable Code editions for each and any additional notes.  For SA/A-516 the entry is on page 1762 of Section II Part A, 2nd volume.


Hope this helps.



From: material...@googlegroups.com <material...@googlegroups.com> on behalf of Prakash Gotimukul <gprak...@gmail.com>
Sent: Tuesday, June 30, 2015 12:57 AM
To: materials-welding
Subject: Re: [MW:23124] Re: ASME UG-10 interpretation
 
Reply all