T
he published literature and service experience with methanol is much more extensive and has shown for some time shows that methanol is a known SCC agent for steel. Water content, various impurities, temperature, and metallurgical condition of the steel determine methanol SCC susceptibility. You may know very well that residual stress/ excessive hardness could trigger SCC.Thanks.