WPS from AWS to BS Standards

702 views
Skip to first unread message

Hani Al Masry

unread,
Oct 15, 2020, 9:17:19 AM10/15/20
to material...@googlegroups.com
Dear Experts 

Our client is asking to convert our WPS from AWS to BS Standards
can you please advise 
which BS standards we need to use 
what the mean steps to be changed according to this BS 
Requirement of back stip for pipe welding 

Regards,
H.A

Vinoth Rajendran

unread,
Oct 15, 2020, 11:29:44 PM10/15/20
to material...@googlegroups.com
Please go through EN  ISO 15609, EN ISO 15614-1, EN ISO 9606

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzfjuGE1OGLGRz%2B7gY0syR5F8ifC9jRFWdyzzR3n7bZDXA%40mail.gmail.com.

Hani Al Masry

unread,
Oct 16, 2020, 11:50:23 PM10/16/20
to material...@googlegroups.com
 
how about 

·                  BS EN ISO 15614-1 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys


what is the major changes i need to made to the current WPS to convert it from AWS to 



Hani Al Masry

unread,
Oct 20, 2020, 10:43:14 AM10/20/20
to material...@googlegroups.com
Dear  Vinoth / Experts 

i had prepared preliminary WPS as per  ISO 15614-1  so please check all parameters and inputs are ok or not 

additionally , check if this cover welding positions up to 6G and steel grade S355 and thickness up to 32mm 

Appreciate your fast action and assistance 

Regards,
H.A
1.WPS-ACFY-03 Rev00-ISO 15614-1-2020-10-18.pdf

Mayur Hiremath

unread,
Oct 20, 2020, 11:19:00 AM10/20/20
to material...@googlegroups.com
Hello, 

PG will not cover 6G, Refer attached Welding positions.

Also need to change the Current , voltage according to Consumable Manufacturer Data sheet as per the thickness of electrodes. Then heat input <=3KJ/mm.
When preparing pWPS parameters need to consider as per data sheet of consumable.
Regards,

IMG_20201020_190334.jpg

Hani Al Masry

unread,
Oct 20, 2020, 11:38:22 PM10/20/20
to material...@googlegroups.com
Welding position here is as per ISO 15614-1 Not AWS D1.1 as i said before and clearly mentioned in WPS and subject title 
as per ISO 15164-1 
image.png
This means only PG and H-LO45 need to be separately qualified , and if qualified for any position all other position will be qualified except PG and HI-LO45 
My case here in over head welding (5G See below Sketch ) so PG will cover all position expect HI-LO45 
image.png

For Current and voltage this values are taken already from actual WPS/PQR but according to AWS D1.1 as i told you i need only to convert it to BS EN 
this Preliminary WPS as you know actual values will be recorded and written during running of final PQR 
Trade name and brand is not mandatory variable here too 

Hope it is clear now 

Regards,
H.A


Vinayak Naik

unread,
Oct 21, 2020, 10:13:12 AM10/21/20
to material...@googlegroups.com
Can any one tell me how to read this?

IMG_20201021_182936208.jpg

Mayur Hiremath

unread,
Oct 21, 2020, 10:36:41 AM10/21/20
to material...@googlegroups.com
Kindly send your AWS WPS with PQR, let look into details and get back to you.

Reply all
Reply to author
Forward
0 new messages