Dear frnds
For hydro test limit contractor does not have any blind flange or end caps so contractor requesting to diectly weld blind to the pipe. Is it acceptable. Any references for that. Constrtion code b31.3 test pressure 44 kgf per cm square
Regards
Jayasuryan
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGt3MynrnPY%3D3LPhP2tw2s2c_s3tTGb410uvn7o1bbVyCqM75w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
| Yes blind can be welded directly to pipe but check the thickness of blind. Sent from Yahoo Mail on Android
|
|
Dear it is not acceptable at all. Pl ask for the required standard and Specs which is valid as per the B31.1.
Peter
Welding Eng.
--
In b31.3 its mentioned only using blanks and spades ,not welded blanks.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55c35a77.691db50a.956bf.205aSMTPIN_ADDED_BROKEN%40gmr-mx.google.com.
Dear frnds
In design point of view is it acceptable. The weld joint will withstand the test pressure. ?
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1438873073.34513.YahooMailAndroidMobile%40web181303.mail.ne1.yahoo.com.