Dear sirs,
  
        Please give me the requirements of the PWHT thickness ranges of Carbon steel materials

José Juan Jiménez Alejandro

未读,
2020年10月30日 21:06:362020/10/30
收件人 material...@googlegroups.com
Construction Code?

El mié., 28 de octubre de 2020 11:40 p. m., Sujith Murali Issac <sujit...@gmail.com> escribió:
Dear sirs,
  
        Please give me the requirements of the PWHT thickness ranges of Carbon steel materials

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5ade924c-7b40-4912-9adc-62dbf868df3dn%40googlegroups.com.

Sujith Murali Issac

未读,
2020年10月31日 02:55:032020/10/31
收件人 material...@googlegroups.com
ASME SEC VIII DIV 1 AND ASME SEC 1

Jamie Reyes

未读,
2020年10月31日 10:09:222020/10/31
收件人 material...@googlegroups.com
Greetings. Please specify the code of construction. If you would like an example, one could review ASME Section VIII Division 1; UW-40; UCS-56; Table UCS-56-1 for Post weld HeatTreatment Requirements of Carbon and Low Alloy Steels (P-No. 1)
Cheers.....
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

Bien_ND

未读,
2020年11月1日 05:37:242020/11/1
收件人 Materials & Welding
It is followed construction codes and material application. Yes, it is different by service or design.