to Materials & Welding
If weep hole is not provided in dummy pipe before welding
What will happen???

atul khatri

unread,
Sep 9, 2019, 6:58:19 AM9/9/19
to material...@googlegroups.com
Hi raghul,
Weep hole in dummy pipe is to vent out the heat and gases during welding.
you can have the weep hole in base plate as well.

On Mon, Sep 9, 2019 at 3:57 PM Raghul <raghul...@gmail.com> wrote:
If weep hole is not provided in dummy pipe before welding
What will happen???

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com.

Raghul

unread,
Sep 10, 2019, 12:31:10 AM9/10/19
to Materials & Welding
I know the purpose of weep hole

But what I am asking is,If weep hole not provided
What is the problem will come ??

atul khatri

unread,
Sep 10, 2019, 7:18:58 AM9/10/19
to material...@googlegroups.com
The trapped burnt gases may be corrosive and corrode the weld joint and dummy pipe in due course.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages