Dear Experts, please confirm if plate 3G welding can be used to perform PQR for a 6G
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4SF2pzp_dB4Qp0aBKsm%3D82odEd8DGReLJ4eEK_iEf8CZw%40mail.gmail.com.
On Jun 19, 2023, at 12:16, Keribo Berepele <bere...@gmail.com> wrote:
please can i site it in any where, document please
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-jw2s8%2B3zprob6YSY8xQ%3Dnhb8gR0bO67pAJDO7hgiazHw%40mail.gmail.com.
Dear Experts, please confirm if plate 3G welding can be used to perform PQR for a 6G
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4SF2pzp_dB4Qp0aBKsm%3D82odEd8DGReLJ4eEK_iEf8CZw%40mail.gmail.com.
![]() |
| |
TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies. The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments. | ||
Your Analysis is correct but let me ask you a question?ASME IX QW 211, states that's "Base metal may consist of either PLATS, PIPES or other product forms. Qualification in plate also qualifies for pipe welding and vice versa" Now plate and pipes are different positions and material therefore using pipe to qualify plates and plates to qualify for pipes ordinarily means that at the point of qualification the position is not an essential variable.. if it does why did the ASME say so on qualification test coupon. I know that position is an essential variable when it is for production weld.Please clarify more on this also. Thanks for your support