PQR

117 views
Skip to first unread message

Keribo Berepele

unread,
Jun 19, 2023, 6:30:09 AM6/19/23
to material...@googlegroups.com
Dear Experts, please confirm if plate 3G welding can be used to perform PQR for a 6G 

Ritesh Kumar Singh

unread,
Jun 19, 2023, 6:55:13 AM6/19/23
to material...@googlegroups.com
Yes You can  position is non essential variable in WPS.

On Mon, 19 Jun 2023, 4:00 PM Keribo Berepele <bere...@gmail.com> wrote:
Dear Experts, please confirm if plate 3G welding can be used to perform PQR for a 6G 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4SF2pzp_dB4Qp0aBKsm%3D82odEd8DGReLJ4eEK_iEf8CZw%40mail.gmail.com.

Keribo Berepele

unread,
Jun 19, 2023, 11:17:22 PM6/19/23
to material...@googlegroups.com
 Thanks I see QW 211 ASME IX that explain for the material 

Sent from my iPhone

On Jun 19, 2023, at 12:16, Keribo Berepele <bere...@gmail.com> wrote:


please can i site it in any where, document please

Mostafa DAIF

unread,
Jun 19, 2023, 11:17:22 PM6/19/23
to material...@googlegroups.com
Hi,

No, a 3G welding qualification cannot be used to perform PQR (Procedure Qualification Record) for a 6G welding position. The reason lies in the welding positions themselves.

The 3G position is a vertical welding position, where the welding is performed on a vertical plate with the weld axis in the vertical position. While a welder qualified in the 3G position demonstrates the ability to weld in the flat (1G), horizontal (2G), and vertical (3G) positions, it does not cover all positions.

The 6G position, on the other hand, is a more complex welding position that covers pipe welding in an inclined, fixed position (with the pipe axis at a 45-degree).

Because the 6G position encompasses a wider range of welding positions and requires greater skill, a welder qualified in the 3G position alone cannot be used to perform PQR for a 6G welding position. Instead, the welder would need to obtain a separate qualification for the 6G position to demonstrate their ability to perform welding in that specific position.

It is essential to have the appropriate qualifications for each welding position, as they are designed to ensure weld quality, safety, and structural integrity.

Le lun. 19 jui. 2023 à 13:30, Keribo Berepele <bere...@gmail.com> a écrit :
Dear Experts, please confirm if plate 3G welding can be used to perform PQR for a 6G 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4SF2pzp_dB4Qp0aBKsm%3D82odEd8DGReLJ4eEK_iEf8CZw%40mail.gmail.com.
--

Mostafa DAIF
Chef preparateur

T : 05 23 38 90 72
M : 06 61 54 12 95
TAQA MOROCCO PB 99 Sidi Bouzid - El Jadida 24 000 - Maroc
taqamorocco.ma

TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies.
  

The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments.


Keribo Berepele

unread,
Jun 20, 2023, 4:49:31 AM6/20/23
to material...@googlegroups.com
Kindly see attached, this was approved by 3rd party inspection agents but my client is having a different thought as Plates can not be used for PQR for pipes remember QW 211. 

On Tue, Jun 20, 2023 at 7:55 AM Keribo Berepele <bere...@gmail.com> wrote:
Your Analysis is correct but let me ask you a question?
ASME IX QW 211, states that's "Base metal may consist of either PLATS, PIPES or other product forms. Qualification in plate also qualifies for pipe welding and vice versa" Now plate and pipes are different positions and material therefore using pipe to qualify plates and plates to qualify for pipes ordinarily means that at the point of qualification the position is not an essential variable.. if it does why did the ASME say so on qualification test coupon. I know that position is an essential variable when it is for production weld.
Please clarify more on this also. Thanks for your support

PQR.pdf

james gerald

unread,
Jun 20, 2023, 6:09:36 AM6/20/23
to material...@googlegroups.com
Properties of welding are governed by Welding parameters and all other essential variables as listed In ASME Sec.iX for each welding process. If essential variables have complied then you obtain a Good weld.

The position is a supplementary essential variable (progression up or down) and change in position only tests the skill of the welder governed by WElder Qualification (Refer QW-461.9)

Thanks & Regards

J.Gerald Jayakumar0091-8838619635