Materials come with solution annealed/ annealed conditions, consumables do not.
Any way ER NiCr-3 is being advised.
Thanks
Regards,
Manish kulkarni
--------------------------------------------
On Sun, 21/2/16, Ramin Kondori <
ramink...@gmail.com> wrote:
Subject: Re: [MW:24340] dissimilar weld
To:
material...@googlegroups.com
Date: Sunday, 21 February, 2016, 9:30 PM
if 625
meets your service requirements, so will ERNiCrMo-3What
I mean is that this filler metal matches the properties of
625 quite well...So if 625 is fit for this
service, ERNiCrMo-3 could be acceptable
too...
Ramin
KondoriSr. QA/QC & Welding
Engineer-----------------------------------------------------------PG-Dip. in Welding
Engineering (IWE AT 0070)BSc. in Civil Engineering
(IUT)BGAS Painting
InspectorASNT Level
I&II
On Sun, Feb 21, 2016 at
4:38 PM, manish kulkarni <
kul_m...@yahoo.co.in>
wrote:
But there
are limitations for temp. In spur service for this
consumable.
Sent
from Yahoo Mail on Android
On Sun, 21
Feb, 2016 at 4:13 pm, Ramin Kondori<
ramink...@gmail.com>
wrote: ER NiCrMo-3 will do
the gob
Ramin
KondoriSr. QA/QC & Welding
Engineer-----------------------------------------------------------PG-Dip. in Welding
Engineering (IWE AT 0070)BSc. in Civil Engineering
(IUT)BGAS Painting
InspectorASNT Level
I&II