Dear all,
Shall we used E6010 electrode for root for 31.3 process piping?
Is there restriction specifies in B31.3?

ishwar kumar

未読、
2017/03/21 1:21:522017/03/21
To: material...@googlegroups.com
Yes we can 

Sent from my iPhone
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANX-_HGuYG7KiBuz4xc-9VhQJ%2BNNOANujkoLsgZDBGEgBjsQ0w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Dinesh Somwanshi

未読、
2017/03/21 6:57:272017/03/21
To: material...@googlegroups.com

You can use. High welders required as to control root penetration. Chances of more burn through

Thanking You,

With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

On Mar 21, 2017 2:21 PM, "ishwar kumar" <ish...@gmail.com> wrote:
Yes we can 

Sent from my iPhone

On 21-Mar-2017, at 12:39 AM, S.Mohammed <mohd...@gmail.com> wrote:

Dear all,
Shall we used E6010 electrode for root for 31.3 process piping?
Is there restriction specifies in B31.3?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/21B46305-39B6-4FD8-B538-96EF51C12FDC%40gmail.com.

Kannayeram Gnanapandithan

未読、
2017/03/21 6:57:302017/03/21
To: materials-welding
no because it has got more H2 of 30to60ppm

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Mar 21, 2017 at 10:29 AM, ishwar kumar <ish...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (ish...@gmail.com) Add cleanup rule | More info

Yes we can 

Sent from my iPhone

On 21-Mar-2017, at 12:39 AM, S.Mohammed <mohd...@gmail.com> wrote:

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANX-_HGuYG7KiBuz4xc-9VhQJ%2BNNOANujkoLsgZDBGEgBjsQ0w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

muthu barathi

未読、
2017/03/22 2:48:192017/03/22
To: material...@googlegroups.com


Dear Sir,

In process piping B 31.3 for larger dia we use E6010 for so many years. Fumes shall be safely exhausted.



Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +9184695933

Sent from RediffmailNG on Android





From: Kannayeram Gnanapandithan <kgpan...@gmail.com>
Sent: Tue, 21 Mar 2017 16:27:30 GMT+0530
To: materials-welding <material...@googlegroups.com>
Subject: Re: [MW:26238] E6010 electrode for root

no because it has got more H2 of 30to60ppm

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Mar 21, 2017 at 10:29 AM, ishwar kumar <ish...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (ish...@gmail.com) Add cleanup rule | More info

Yes we can 

Sent from my iPhone

On 21-Mar-2017, at 12:39 AM, S.Mohammed <mohd...@gmail.com> wrote:

Dear all,
Shall we used E6010 electrode for root for 31.3 process piping?
Is there restriction specifies in B31.3?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMpESBbrnZ=rQ1UPj6NfhwknB5MDbZqWL1Vza=RTS...@mail.gmail.com.

muthu barathi

未読、
2017/03/22 2:58:092017/03/22
To: material...@googlegroups.com


Dear Sir,

For larger bore E6010 shall be used as it gives deep penetrationbecause of it is shielded with cellulose flux. There is no restriction in B31.3 for using E6010.


Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +9184695933

Sent from RediffmailNG on Android




From: Dinesh Somwanshi <som...@gmail.com>
Sent: Tue, 21 Mar 2017 16:27:27 GMT+0530
To: material...@googlegroups.com
Subject: Re: [MW:26238] E6010 electrode for root

You can use. High welders required as to control root penetration. Chances of more burn through

Thanking You,

With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

On Mar 21, 2017 2:21 PM, "ishwar kumar" <ish...@gmail.com> wrote:
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrV31noJ3nLG4ROfEav_...@mail.gmail.com.

Alpesh Sakhreliya

未読、
2017/04/02 3:16:542017/04/02
To: material...@googlegroups.com
I would like to inform that E6010 mainly use in pipeline project 

E6010 only for Pipeline b'caz of this electrodes down hill process 
Stations piping always uphill process




For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.