Diff. between WPS of SEC-IX and AWS D1.1

3,886 views
Skip to first unread message

Ramesh Barot

unread,
May 6, 2011, 5:54:15 AM5/6/11
to Materials Welding

Dear Experts,

 

Greetings,

 

I have one basic question about WPS.

 

Please share your valuable opinions with me that Difference between qualification of WPS with AWS D1.1 and ASME -IX.

 

Can we use the WPS qualified with SEC-IX for steel structure and vise versa?

 

 

Thanks,
With Best Regards,
Ramesh Barot

anilkumar

unread,
May 19, 2011, 7:06:38 AM5/19/11
to Materials & Welding
ASME- Scen. IX-- exclusively for pressure vesel
AWS D1.! - Meant for Structural welding code
No, We can not use WPS qualified with SEC-IX for steel structure and
vise

Thanks

On May 6, 2:54 pm, Ramesh Barot <rameshnba...@yahoo.com> wrote:
> Dear Experts,
>  
> Greetings,
>  
> I have one basic question about WPS.
>  
> Please share your valuable opinions with me that Difference between
> qualification of WPS with AWS D1.1 and ASME -IX.
>  
> Can we use the WPS qualified with SEC-IX for steel structure and vise versa?
>  
>  
> Cell+919978917399Thanks,

Karthik

unread,
May 20, 2011, 1:01:42 AM5/20/11
to material...@googlegroups.com
Hi,
Pls.find below the extraction of AWS and ASME Sec.IX.According to that,Sec.IX WPS may not be used for AWS. But AWS SWPS can be used for ASME as per QW-100.1.
AWS -
4.1.1.2 WPS Qualification to Other Standards.

The acceptability of qualification to other standards is

the Engineer’s responsibility, to be exercised based upon

the specific structure, or service conditions, or both.

AWS B2.1.XXX-XX Series on Standard Welding Procedure

Specifications may, in this manner, be accepted for

use in this code.
 
ASME-Sec-IX

QW-100.1

A Welding Procedure Specification (WPS)

is a written document that provides direction to the welder

or welding operator for making production welds in accordance

with Code requirements. Any WPSs used by a manufacturer

or contractor that will have responsible operational

control of production welding shall be a WPS that has

been qualified by that manufacturer or contractor in accordance

with Article II, or it shall be an AWS Standard

Welding Procedure Specification (SWPS) listed in Appendix

E and adopted by that manufacturer or contractor in

accordance with Article V.

Both WPSs and SWPSs specify the conditions (including

ranges, if any) under which welding must be performed.

These conditions include the base metals that are permitted,

the filler metals that must be used (if any), preheat and

postweld heat treatment requirements, etc.

Such conditions are referred to in this Section as welding “variables.”



Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 5/19/11, anilkumar <anil...@gmail.com> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Prasad Joshi

unread,
Jun 9, 2011, 6:38:32 PM6/9/11
to material...@googlegroups.com
I feel you can use the WPS qualified with Sec.IX for the structural parts of the pressure vessels/piping provided the AWS D1.1 is not used for design of the structure. I remember the design code (Sec.VIII/ASME B31.3) gives such permission.
 
But if the structure is designed as per AWS D1.1 (like, process platform or bridges, etc. where the provisions of D1.1 are used  for designing, then you cannot use the WPSqualified by ASME Sec. IX.
 
The codes are far different in their qualification strategy.
 
I hope this may be useful,
 
Prasad Joshi
Linde

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com

Shashank Vagal

unread,
Jun 10, 2011, 10:30:57 AM6/10/11
to material...@googlegroups.com
However, look at the PQR parameters and see if it can be re-presented in the new required format. sometimes it can be re-used to suit the other code requirements and a new WPS.

--- On Fri, 10/6/11, Prasad Joshi <sur...@gmail.com> wrote:

Shaik Basha

unread,
May 27, 2014, 11:20:43 PM5/27/14
to material...@googlegroups.com
Dear Ramesh,

WPSs qualified to ASME IX code is allowed for AWS D1.1 welding with consent of buyer as stated in AWS D1.1 - 2010 clause 4.2.1.2.

Moreover, the structure designed as per AWS will not be subjected to similar type of integrity tests as per ASME Sec VIII/B31.3/31.1 because ASME is for pressure vessels, boilers etc.

Hope this will help.

Shaik Basha

unread,
May 28, 2014, 3:30:50 AM5/28/14
to material...@googlegroups.com
Dear Ramesh,

WPSs qualified to ASME IX code is allowed for AWS D1.1 welding with consent of buyer as stated in AWS D1.1 - 2010 clause 4.1.1.2.

Moreover, the structure designed as per AWS will not be subjected to similar type of integrity tests as per ASME Sec VIII/B31.3/31.1 because ASME is for pressure vessels, boilers etc.

Hope this will help.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/

 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/l2-aZsX_AGo/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

veera raghava kommisetti

unread,
May 28, 2014, 3:32:11 AM5/28/14
to material...@googlegroups.com
Referencing codes shall be used in conjunction with code of construction.
It all depends on Code of Construction. Some codes permit use of both codes/standards.


On Wed, May 28, 2014 at 7:20 AM, Shaik Basha <shai...@gmail.com> wrote:

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

kannayeram gnanapandithan

unread,
May 28, 2014, 3:32:25 AM5/28/14
to materials-welding
AWS D1.1 is more stringent than ASME sec 9 regarding position and so on . Ref 4.1.1.2

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


--

Ramin Kondori

unread,
Jun 1, 2014, 11:25:22 PM6/1/14
to material...@googlegroups.com
Dear Ramesh:

As Shashank said, you can use it if it reflects you actual welding conditions and PQR includes required tests and results. But this is always the engineer's decision (it's better to receive client's approval). If there are reasonable justifications, go ahead and use it.

Best Regards

Ramin Kondori

Sr. QA/QC engineer

Yadavaran Oilfield Project

SIPC (SINOPEC)