ucs 56 adress minimum holding temprature eg- for Pno 1 its 595 C. can i hold it at temp 915℃ because after 915 there will be change from alpha phase to gamma and bcc structure to fcc.
and one more point from 770c there will be also change from magnetic to non magnetic property.

i take refference from iron carbon diagram.

rajesh kaswala

unread,
Nov 25, 2018, 9:35:49 PM11/25/18
to material...@googlegroups.com
595 for pwht , 915 normalizing 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Er Sourav Bohray

unread,
Nov 25, 2018, 10:16:36 PM11/25/18
to material...@googlegroups.com
wrong i did pwht at 623 for my vessel already

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/_TDdsZG7EfI/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

munee...@gmail.com

unread,
Nov 26, 2018, 11:30:22 PM11/26/18
to materials-welding
refer 27-7, you can take that clause lieu for ucs-56 on the whole 27-7s condition, only if you have that specific requirements.

Thanks

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
munee...@gmail.com +91-636-955-7189

(55:33) O company of jinn and men, if you have the power to go beyond the bounds of the heavens and the earth, go beyond them! Yet you will be unable to go beyond them for that requires infinite power.

Reply all
Reply to author
Forward
0 new messages