acceptance edition of asme

265 views
Skip to first unread message

Souravbohray

unread,
Jul 14, 2018, 1:55:12 AM7/14/18
to Materials & Welding
can i use raw material based on asme sec 2 part A edition 2015 even asme 2017 edition already published

Prasad Ghanekar

unread,
Jul 14, 2018, 3:33:57 AM7/14/18
to material...@googlegroups.com
Yes.
You need to compare with 2017 edition, if found fulfilling all mandatory requirements then you have to recertify as 2017.

On Sat, 14 Jul 2018 11:25 Souravbohray, <ermechsou...@gmail.com> wrote:
can i use raw material based on asme sec 2 part A edition 2015 even asme 2017 edition already published

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Nithin Joseph

unread,
Jul 14, 2018, 6:20:30 AM7/14/18
to material...@googlegroups.com
For ASME Code works,

You need to check the acceptable adopted ASTM editions for the subject material, if its same then just review as per 2017 and sign off. If both ASTM editions are different, they you might have to do a thorough review of the both ASTM standards to ensure it is not affecting your material. You have to perform additional tests if required to meet new standards requirements if any. This review you have to document, as part of your system.

On Sat, Jul 14, 2018 at 11:23 AM, Prasad Ghanekar <prs...@gmail.com> wrote:
Yes.
You need to compare with 2017 edition, if found fulfilling all mandatory requirements then you have to recertify as 2017.
On Sat, 14 Jul 2018 11:25 Souravbohray, <ermechsou...@gmail.com> wrote:
can i use raw material based on asme sec 2 part A edition 2015 even asme 2017 edition already published

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.



--
Regards,
Dsilva

Er Sourav Bohray

unread,
Jul 14, 2018, 6:20:35 AM7/14/18
to material...@googlegroups.com
but sr asme sec 2 part A table 200 give info that accepted edition for sa516 gr70 is upto only 2010 .except 2017 edition i can only use edition upto 2010.

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/XwdP_oqBRaY/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

Ramesh

unread,
Jul 26, 2018, 2:59:53 PM7/26/18
to material...@googlegroups.com

Hi

I am unable to understand your question fully. 

 

Your plate is already produced / certified  before issuing  2017 edition, you can’t do anything.

 

Even, Supplier can’t provide you same MTC with same heat number or batch numbers !!!

 

Pl refer attached screen shot from “Sec IIA-P2 mandatory appendix ii Basis for use of acceptable asme, astm, and non-astm Editions” which may be helpful .

 

Anyway, you can use that raw material said by earlier members on this topic




Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"


On Sat, Jul 14, 2018 at 1:36 PM, Er Sourav Bohray <ermechsou...@gmail.com> wrote:
but sr asme sec 2 part A table 200 give info that accepted edition for sa516 gr70 is upto only 2010 .except 2017 edition i can only use edition upto 2010.
On 14 Jul 2018 1:03 p.m., "Prasad Ghanekar" <prs...@gmail.com> wrote:
Yes.
You need to compare with 2017 edition, if found fulfilling all mandatory requirements then you have to recertify as 2017.

On Sat, 14 Jul 2018 11:25 Souravbohray, <ermechsou...@gmail.com> wrote:
can i use raw material based on asme sec 2 part A edition 2015 even asme 2017 edition already published

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/XwdP_oqBRaY/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Pages from BPVC-IIA-2_2017.pdf

Souravbohray

unread,
Jul 27, 2018, 1:43:30 AM7/27/18
to Materials & Welding
yes asme sec2 part A table no 200 is given in which accept year of edition is provided.

George Dilintas

unread,
Sep 23, 2018, 10:24:01 PM9/23/18
to Meghanadh K
check table II-200-1 in the mandatory appendices of Section II-A

Στις Σάβ, 14 Ιουλ 2018 στις 8:55 π.μ., ο/η Souravbohray <ermechsou...@gmail.com> έγραψε:
can i use raw material based on asme sec 2 part A edition 2015 even asme 2017 edition already published

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Aslam Khan

unread,
Sep 24, 2018, 2:54:49 AM9/24/18
to material...@googlegroups.com
You can use older variable supported by older pqr but for new wps , new pqr is required...