Vanadium composition showing in p91

83 views
Skip to first unread message

mithlesh kumar

unread,
Dec 17, 2022, 9:45:23 AM12/17/22
to Materials & Welding
Dear team,

I have observed vanadium in heat analysis of p91 MTC  , but as per code vanadium is not showing in chemical composition table. Suggest is it acceptable or not if acceptable code reference please.

mithlesh kumar

unread,
Dec 17, 2022, 10:17:13 AM12/17/22
to Materials & Welding
Kindly read WP22 instead of P91

Vishwas Keskar Welding Manager WELDING

unread,
Dec 18, 2022, 10:13:38 PM12/18/22
to Materials & Welding
What is the % Vanadium in that MTC ?
It is trace elements not a deliberate addition for Gr 22  unlike Gr 91 where it it MUST in Gr 91 

Regards

Vishwas IWE
International Welding Engineer 

mithlesh kumar

unread,
Dec 18, 2022, 10:24:33 PM12/18/22
to material...@googlegroups.com
Vandium % is .004

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/UmVRYgreKIE/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1f2331d9-3cb1-437c-adc3-ba7b8be6f9f8n%40googlegroups.com.

Kannayeram Gnanapandithan

unread,
Dec 19, 2022, 4:31:56 AM12/19/22
to material...@googlegroups.com
P/T 91 is CrMov steel
It should have Vanadium  and it is a precipitation hardening elements.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Vishwas Keskar Welding Manager WELDING

unread,
Dec 19, 2022, 4:32:01 AM12/19/22
to Materials & Welding
0.004 % V- its trace element  
Not a deliberate addition


mithlesh kumar

unread,
Dec 19, 2022, 10:19:33 PM12/19/22
to Materials & Welding

Sir please read WP22 instead of P91

james gerald

unread,
Dec 20, 2022, 3:10:14 AM12/20/22
to material...@googlegroups.com
Gentleman,

SA234 WP22 is for 2.25Cr-1Mo steel

where as P91 is modified 9Cr-1Mo steel with additions of Nb and V which provides higher creep strength at applicable higher temperatures and which differentiates from P9 steel (9Cr-1M0).

See below snap shot

Inline image

Thanks & Regards

J.Gerald Jayakumar




Reply all
Reply to author
Forward
0 new messages