Dear Experts,

What is P-No. of UNS 06626, my client say its P No.45 but that materials simillar with UNS 06625 which is its P-No.43. Please for the advice

Thanks

Mostafa DAIF

unread,
Feb 28, 2024, 5:57:15 AM2/28/24
to material...@googlegroups.com
Dear all,
The P number is P42 according to ASME Boiler & Pressure Vessel Code Section IX;

Best Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c105a43f-72c7-44b6-96e1-0e11095552a3n%40googlegroups.com.


--

Mostafa DAIF
Chef preparateur

T : 05 23 38 90 72
M : 06 61 54 12 95
TAQA MOROCCO PB 99 Sidi Bouzid - El Jadida 24 000 - Maroc
taqamorocco.ma

TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies.
  

The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments.


cyndiso yapi

unread,
Feb 28, 2024, 5:57:20 AM2/28/24
to material...@googlegroups.com
Its P-No 43 check ASME IX Table QW422 it's listed there 

--

Chiranjeevi A

unread,
Feb 28, 2024, 5:57:31 AM2/28/24
to material...@googlegroups.com
Dear Fauzi,

Please refer to the Limiting chemical composition in MTC & concerning ASME Code Case 2276 
It should be P-No. 43



--

Chiranjeevi A

unread,
Feb 28, 2024, 8:29:11 AM2/28/24
to material...@googlegroups.com
Dear all,

Please refer to the table below for the required chemical composition of UNS 06626 under case 2276, as per the ASME BPV code cases. The P-No. for material UNS 06626 is P-43.

image.png

ilham fauzi

unread,
Feb 29, 2024, 12:35:04 AM2/29/24
to material...@googlegroups.com
Dear All Experts,

Thanks all for the advice and information. I checked ASME code case 2276-1, which states that UNS 06626 can be classified as category P-No.43.
image.png
Thanks a bunch.

Best Regards,
M Ilham Fauzi Pane
Welding Engineer


You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/SpmpHXyXbjw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zYAakAwiLyp2J3AqpDMTSFAhCZXPSKUY5ZFFYy2gTh8Q%40mail.gmail.com.

Vinay

unread,
Mar 25, 2024, 5:18:18 AM3/25/24
to material...@googlegroups.com
PL confirm , it is UNS N06626 . Its Ni-Cr moly steel..   P-45 is correct.
P-43 is for Inconel 625 i.e UNS 06625 . 

--

saleem manhappulath

unread,
Oct 23, 2024, 5:59:16 AM10/23/24
to material...@googlegroups.com
Dear Team

   KINDLY SUGGEST PREHEAT TEMP. MIN. AND MAX. FOR INC625

 
Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936


sridhar cn

unread,
Oct 24, 2024, 12:33:56 AM10/24/24
to material...@googlegroups.com
Mr. Saleem, 
Incl 625,minimum preheat temp. should be 50 deg. C and should not cross 200 deg. C.  Interpass temp. should not 
exceed 250 deg. C to avoid effects on material integrity  and mechanical properties. 
Generally, Preheat is not required  for incl 625. This range will help to reduce the thermal shocks in thicker sections, 
control the cooling rates, provide good weldability, and to prevent cracking during cooling. Heat-input to be controlled 
to avoid grain growth and reduced toughness.

C Sridhar.
-----------------------------------------------------------------------------------------------

sridhar cn

unread,
Oct 24, 2024, 10:35:37 AM10/24/24
to material...@googlegroups.com
P. no for UNS 06626 (inconel 625 LCF) is P45 and UNS 06625 (inconel 625) is P43.
Though both are Ni-Cr-Mo based, 06626 has more controlled microstructure for increased fatigue resistance 
at cyclic temperature conditions and is used for bellows and aerospace joints used at elevated temperatures. 
UNS n06625 is used for its high strength and corrosion resistance applications. 
Sridhar.

On Wed, 23 Oct 2024 at 15:29, saleem manhappulath <salee...@gmail.com> wrote:
Reply all
Reply to author
Forward
0 new messages