Want to understand the "Product analysis"

112 views
Skip to first unread message

Umar Rashid Makrani

unread,
Jul 8, 2015, 6:35:52 AM7/8/15
to material...@googlegroups.com
Dear Mentors,
For Material ASTM A516 Gr 70 the client requirement is based on product analysis. Does that mean that all plates shall be tested for product analysis? or certain plates from that heat is enough to report that as product analysis.
Thanks in advance for your kind advise if possible with citation.
Best regards,
Umar.

Umar Rashid Makrani

unread,
Jul 9, 2015, 5:11:45 AM7/9/15
to material...@googlegroups.com
Further,
The client requirement is" S19. Restricted chemistry: Carbon Max 0.2% and Vanadium Max.XX% restricted for heat and product analysis, can I interpret this as a supplementary requirement S2of SA20?

Dark_Horse

unread,
Jul 13, 2015, 12:34:41 PM7/13/15
to material...@googlegroups.com
Product analysis is always on basis of Heat No and it is done on sampling basis.   In case of coils, it is done from drawing sample from both front and tail end of the coil.  for it is illogical to take it from centre of the coil !!!.
If buying from a trader, possible plates may  belong to different heat, then buyer to advice whether they want 100% testing or random samples.

sreeram

Umar Makrani

unread,
Jul 13, 2015, 1:32:39 PM7/13/15
to material...@googlegroups.com
In technical delivery conditions the client mentions 
"S19. Restricted chemistry: Carbon Max 0.2% and Vanadium Max.XX% restricted for heat and product analysis,"

In context of SA20, should the supplementary requirement S2 be invoked?

 

 

Thanks & Regards

 

Firoz Ahmed R. Makrani, PMP®

--
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/NDLX5-JcODk/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/825d64ec-6610-4c26-bc2f-b715b0f09f74%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Shaik Basha

unread,
Jul 20, 2015, 10:40:37 PM7/20/15
to material...@googlegroups.com
Hi
Refer to ASTM A6 AND A 20 for details regarding product analysis

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

Umar Makrani

unread,
Jul 21, 2015, 1:26:15 PM7/21/15
to material...@googlegroups.com
Astm a20 refers supplementary requirement S2. In the context of below mail will S2 invoked?


 

 

Thanks & Regards

 

Firoz Ahmed R. Makrani, PMP®

Sr. Inspection Engineer