Hardness after PWHT

260 views
Skip to first unread message

patelr...@gmail.com

unread,
Jan 14, 2020, 6:58:58 AM1/14/20
to Materials & Welding
Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.

Karthik

unread,
Jan 14, 2020, 7:49:58 AM1/14/20
to material...@googlegroups.com
Hi, 
Please refer Section II Part -A SA 182 . It’s specified


Sent from Yahoo Mail for iPhone


On Tuesday, January 14, 2020, 6:15 PM, patelr...@gmail.com wrote:

Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

Prakash Hegde

unread,
Jan 14, 2020, 10:21:23 PM1/14/20
to material...@googlegroups.com
Hi
Generally BHN235 MAX is acceptable limit after PWHT
Regards
Hegde
On Tue, 14 Jan 2020 at 17:28, patelr...@gmail.com
Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.

Roshan Patel

unread,
Jan 14, 2020, 10:21:24 PM1/14/20
to material...@googlegroups.com
After PWHT for F11 & F22 hardness reduced to 110 HB, it is acceptable ?

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/M27c_onWphw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1766304718.7446033.1579005997404%40mail.yahoo.com.

Karthik

unread,
Jan 15, 2020, 12:00:03 AM1/15/20
to material...@googlegroups.com
Hi,
As per the Code its not acceptable. If hardness is lesser then the Tensile strength might be reduced. Please check on some other locations. small grinding on the surface before take hardness readings.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

E-mail : karthi...@yahoo.com



To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHABvdUjmzBfu0v5sQE8ar6tP8enbEjdteVErZHcEyBkaR8LuA%40mail.gmail.com.

José Juan Jiménez Alejandro

unread,
Jan 15, 2020, 10:33:43 PM1/15/20
to material...@googlegroups.com
You can mention the Code and paragraph where this information is.
Please.



--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





Karthik

unread,
Jan 15, 2020, 11:03:11 PM1/15/20
to material...@googlegroups.com
Hi,
Please find below the extraction from ASME Section II. your hardness value is lesser than the minimum hardness value required by the code.

Inline image


Thanks& Regards,

 

(Karthik)

Karthikeyan.S

E-mail : karthi...@yahoo.com

Dharmesh Mistry

unread,
Jan 16, 2020, 1:17:48 AM1/16/20
to material...@googlegroups.com
Hi,

Para 12.6 (hardness testing - weld procedure qualification and
production) of API RP 582 to be referred.

Regards,
Dharmesh

On Tue, Jan 14, 2020 at 5:28 PM <patelr...@gmail.com> wrote:
>
> Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/22949c81-66b3-46b2-bd4a-5a46a78bc6d2%40googlegroups.com.



--

Thanks, & With Best Regards,



Dharmesh MISTRY

+91 9820735814

pradip kumar Sil

unread,
Jan 17, 2020, 11:25:50 AM1/17/20
to materials-welding
Designer will decide hardness value for the HAZ and WELDMENT