Gas purity checking for Argon, Argon+CO2(Composition), Oxygen, Acetylene and CO2

280 views
Skip to first unread message

Sathish Kumar

unread,
Sep 10, 2018, 6:11:45 AM9/10/18
to Materials & Welding
Dear Experts
I have following concern o below

1. How to check purity for Argon, Argon+CO2(Composition), Oxygen, Acetylene and CO2 gas cylinder.
2. How to check the moisture and dew point temperature for gas contained.
3. What is the standard (ISO or ASTM or EN) for checking gas purity?
4. Any instrument is available for checking gas purity, moisture and dew point?
5. How to ensure gas quality in after welding?


Please clarify the same


Regards
sathish

Kannayeram Gnanapandithan

unread,
Sep 10, 2018, 6:33:04 AM9/10/18
to materials-welding
shaw meter is available to check all
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

sandy

unread,
Sep 12, 2018, 8:03:36 AM9/12/18
to Materials & Welding
There are gas analyser available in market for your query 1, 2 & 4.
For gas purity requirements (point 3), refer ISO 14175.
For point 5, what you mean by gas quality after welding, It shall be verified before welding. 

Regards
Sandeep Kumar

Sathish Kumar

unread,
Sep 12, 2018, 9:47:28 AM9/12/18
to material...@googlegroups.com, sandeep...@gmail.com
Dear Sir
Thank You
Can you refer the gas analyser product name for reference?

On Wed, Sep 12, 2018 at 6:08 PM sandy <sandeep...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (sandeep...@gmail.com) Add cleanup rule | More info
There are gas analyser available in market for your query 1, 2 & 4.
For gas purity requirements (point 3), refer ISO 14175.
For point 5, what you mean by gas quality after welding, It shall be verified before welding. 

Regards
Sandeep Kumar

On Monday, September 10, 2018 at 1:11:45 PM UTC+3, Sathish Kumar wrote:

--
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/JswNONDgDyU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages