Need suggestion

53 views
Skip to first unread message

Chirag Patel

unread,
Dec 13, 2024, 9:42:46 AM12/13/24
to Materials & Welding
I am having WPS impact temperature range with -20 degree. Can i do the welding for -29 degree impact requirement job as per ASME code 

Vishwas Keskar

unread,
Dec 13, 2024, 10:13:23 PM12/13/24
to material...@googlegroups.com, Materials Welding
What is MDMT in drawing ?
Sent from my iPhone

On 13 Dec 2024, at 8:12 PM, Chirag Patel <chira...@gmail.com> wrote:

I am having WPS impact temperature range with -20 degree. Can i do the welding for -29 degree impact requirement job as per ASME code 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/b7446104-f741-424e-8d98-669afa38f068n%40googlegroups.com.

Prakash Hegde

unread,
Dec 14, 2024, 3:31:52 AM12/14/24
to material...@googlegroups.com
No
 you are allowed to use said wps for welding of job having mdmt -20c and warmer
On Fri, 13 Dec 2024 at 20:12, Chirag Patel
I am having WPS impact temperature range with -20 degree. Can i do the welding for -29 degree impact requirement job as per ASME code 

--

Muhammed Shareef

unread,
Dec 14, 2024, 7:29:16 AM12/14/24
to material...@googlegroups.com
Dear Chirag,

It depends on the material and the minimum temperature mentioned in ASME B31.3 (if applicable).

for CS material  criteria to be defined based on the Table 323.2.2 of applicable 31.3 code.


Thanks
Sharief

On Fri, Dec 13, 2024 at 5:42 PM Chirag Patel <chira...@gmail.com> wrote:
I am having WPS impact temperature range with -20 degree. Can i do the welding for -29 degree impact requirement job as per ASME code 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/b7446104-f741-424e-8d98-669afa38f068n%40googlegroups.com.


--

Kind Regards,

 

Muhammed Sharief

QC Supervisor

Tamimi Industrial Services

(Branch of Tamimi Global Co. Ltd.)

Tel: +966 13 341 1391 Ext. 3228

Mobile: +966 539141980

E Mail : mpazha...@al-tamimi.com

Website: www.tamimi-tis.com


james gerald

unread,
Dec 14, 2024, 7:29:20 AM12/14/24
to 'Prakash Hegde' via Materials & Welding
It will be decided based on Thickness, Material specification as sometimes there may be Base Material Impact exemptions.


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



james gerald

unread,
Dec 14, 2024, 9:31:31 AM12/14/24
to 'james gerald' via Materials & Welding
Also specify the Design Code such as ASME B31.3;  -29degC is a general cutoff for carbon steels such as a106Gr.B, A105 etc..

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635

Chirag Patel

unread,
Dec 15, 2024, 2:43:53 AM12/15/24
to material...@googlegroups.com
3 Degree 

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/8IaCKB7qIAc/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/155624C3-3EEC-4939-B0A8-AE96087ACE46%40gmail.com.
Reply all
Reply to author
Forward
0 new messages