i am looking for acceptance criteria according to asme section ix for visual examination

1,406 views
Skip to first unread message

adeel

unread,
Aug 3, 2018, 12:56:10 PM8/3/18
to Materials & Welding
i am looking for acceptance criteria according to asme section ix for visual examination  of cap hight, undercut, lack of fusion, undfill, arc stricke, penteration, root concavity which article of Asme will help me ....?

Souravbohray

unread,
Aug 4, 2018, 3:16:12 AM8/4/18
to Materials & Welding
sorry i think there is no acceptance criteria given for visual inspection. but during visual inspection dimensional and surface should be free of porosity . crack . undercut .incomplete penetration n fusion. than for consider its relevant or non relevant u have to do lpt.

sathishkumar

unread,
Aug 4, 2018, 4:22:33 AM8/4/18
to material...@googlegroups.com
Hi, Please refer QW-194 of section 9 and also owner/client can decide as well.

Regards
Sathish

Sent from my iPhone

> On Aug 4, 2018, at 12:03 PM, Souravbohray <ermechsou...@gmail.com> wrote:
>
> sorry i think there is no acceptance criteria given for visual inspection. but during visual inspection dimensional and surface should be free of porosity . crack . undercut .incomplete penetration n fusion. than for consider its relevant or non relevant u have to do lpt.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.

Er Sourav Bohray

unread,
Aug 4, 2018, 12:01:12 PM8/4/18
to material...@googlegroups.com
ok if cracks porosity dimension spatter etc occur it is not acceptable u didnt observe one word in qw194 - performane ie for welder . weld should be free of surface defects which are not force to use magnify glass. performance nd procedure should be free of surface defect incomplete fusion penetration

Sourav Bohray
Quality Engineer (QA / QC ) and  Welding Engineer - Pressure Vessel and Heat Exchanger
Contact- ermechsou...@gmail.com

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/3zuayXJ0WvM/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

Ramesh

unread,
Aug 6, 2018, 12:14:50 AM8/6/18
to material...@googlegroups.com

Hi

 

Refer Table 7.6 in ASME Sec VIII Div.2 for your reference








Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"


On Sat, Aug 4, 2018 at 2:15 PM, Er Sourav Bohray <ermechsou...@gmail.com> wrote:
ok if cracks porosity dimension spatter etc occur it is not acceptable u didnt observe one word in qw194 - performane ie for welder . weld should be free of surface defects which are not force to use magnify glass. performance nd procedure should be free of surface defect incomplete fusion penetration

Sourav Bohray
Quality Engineer (QA / QC ) and  Welding Engineer - Pressure Vessel and Heat Exchanger
Contact- ermechsou...@gmail.com
On 4 Aug 2018 1:52 p.m., "sathishkumar" <sathis...@gmail.com> wrote:
Hi, Please refer QW-194 of section 9 and also owner/client can decide as well.

Regards
Sathish

Sent from my iPhone


> On Aug 4, 2018, at 12:03 PM, Souravbohray <ermechsou...@gmail.com> wrote:
>
> sorry i think there is no acceptance criteria given for visual inspection. but during visual inspection dimensional and surface should be free of porosity . crack . undercut .incomplete penetration n fusion. than for consider its relevant or non relevant u have to do lpt.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/3zuayXJ0WvM/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Er Sourav Bohray

unread,
Aug 14, 2018, 11:11:35 PM8/14/18
to material...@googlegroups.com
if we r working on asme sec 8 div 1 we cant use asme sec 8 div 2 . its based on divison of code we have to use for project we cant go to another divison.


Sourav Bohray
Quality Engineer (QA / QC ) and  Welding Engineer - Pressure Vessel and Heat Exchanger
Contact- ermechsou...@gmail.com
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/3zuayXJ0WvM/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/3zuayXJ0WvM/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages