WPS of HOT TAPPING

253 views
Skip to first unread message

asghar...@gmail.com

unread,
Dec 4, 2019, 2:55:07 AM12/4/19
to Materials & Welding
Dear All.

If we want to qualify a WPS for hot tapping on pipeline, we shall apply Appendix B of API1104.
But for hot tapping of piping section for qualification of WPS, which code have to be applied, with regard to ASME IX doesn't mention to in service welding?

Regards

Noufal Mc

unread,
Dec 4, 2019, 10:39:31 PM12/4/19
to material...@googlegroups.com
Dear Friend,

please refer article 10, section 4.1.1 in ASME PCC-2 Ed:2015.

Regards 

NOUFAL MC


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1f432d89-8224-49ba-a8f0-fb716bf6a663%40googlegroups.com.

pradip kumar Sil

unread,
Dec 4, 2019, 10:39:31 PM12/4/19
to materials-welding
Applicable code API 1104 Appendix B

--

Ali Asghari

unread,
Dec 4, 2019, 10:39:31 PM12/4/19
to material...@googlegroups.com
Dear All.

I have found the answer of my question.
ASME PCC2 explain and say about in service welding that would be used for hot tapping.

Regards.

--
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/1nVZMJ0WqJo/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages