Is Decladding is required for internal welds on Cladded vessels??

pgoswami

unread,
Jan 10, 2017, 6:01:47 PM1/10/17
to material...@googlegroups.com

Hi Abhisekh,

 

Welding of internals in a clad vessel is very much possible without major removal of clad. If the vessels is subjected to PWHT and clad restoration is done after PWHT fabricators would like avoid any further welding & PWHT  of the substrate material.

 

What’s is the clad metallurgy including Grade of BM involved?

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist.

Ontario,Canada.

ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

To post to this group, send email to material...@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8a083148-7f83-490f-a798-468f52758517%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

ABHISHEK SINGH

unread,
Jan 13, 2017, 2:39:00 AM1/13/17
to Materials & Welding
Sir inconel 625 Clad on SA516 Gr.65

George Dilintas

unread,
Jan 16, 2017, 10:46:08 AM1/16/17
to Meghanadh K
Ι would not remove the cladding. I would position the internals, mark the areas where internals are touching the cladding, then I would groove the cladding around those marks, and I would weld the internals on the base metal and the cladding with Inco 625

2017-01-11 20:07 GMT+02:00 ABHISHEK SINGH <mech....@gmail.com>:
Sir inconel 625 Clad on SA516 Gr.65
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1c478ccf-28f9-4b65-97dd-c1ce97408d91%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

George Dilintas

unread,
Jan 16, 2017, 10:46:41 AM1/16/17
to Meghanadh K
if you could send a sketch and info on base metal and clad material I could give you some ideas

2017-01-08 19:26 GMT+02:00 ABHISHEK SINGH <mech....@gmail.com>:
Dear Experts,

  Is Decladding is required for internal welds on Cladded vessels??
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

Prakash Hegde

unread,
Jan 16, 2017, 10:47:43 AM1/16/17
to material...@googlegroups.com

Hi!
The  query /question is not clear???


On Tuesday, 10 January 2017 11:42 AM, ABHISHEK SINGH <mech....@gmail.com> wrote:


Dear Experts,
   
  Is Decladding is required for internal welds on Cladded vessels??

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

srinivas rao

unread,
Jan 20, 2017, 4:31:11 AM1/20/17
to Materials & Welding
Dear Abhishek,
Not require
provided appilicable WPS in place.

Regards,
Srinivas