Dear experts

What's the Acceptance of tungsten inc.
According to 1104?
Method: RT

Regards

LALU RAJENDRAN

unread,
Aug 24, 2015, 2:57:29 AM8/24/15
to material...@googlegroups.com
​​Tungsten inclusion is not defined as a defect as per API 1104, however it is often considered a volumetric imperfection and is accepted or rejected accordingly.

regards,
LALU


LALU



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f43bf2b3-c38d-4fd1-b4ad-b2ae6d24a18a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages