Root concavity

140 views
Skip to first unread message

rizwanm...@gmail.com

unread,
Jun 9, 2020, 11:08:01 AM6/9/20
to Materials & Welding
What is the main reasons of coming root concavity or suckback, and who is much responsible for this root hot Welder or filling capping welder?
Thanks

Rajnish Dixit

unread,
Jun 10, 2020, 6:19:01 AM6/10/20
to Materials & Welding
Dear Rizwan,

There may be many reasons for root concavity or suck back appearance in weld joints but exact reasons might be found by analysis based on minimum following aspects:
1. Joint design
2. Size Vs Root gap
3. Welding Process
4. Gas flow
5. Welding Speed
6. Current used
7. Welder’s Technique
8. Position
9. Skill of welder

Thanks,
Best Regards,
Rajnish Dixit

On Tuesday, 9 June, 2020, 10:15:20 pm GMT+7, <rizwanm...@gmail.com> wrote:


What is the main reasons of coming root concavity or suckback, and who is much responsible for this root hot Welder or filling capping welder?
Thanks

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages