Welding between SS304L to IS-2062(CS)

13 views
Skip to first unread message

PARESH JADAV

unread,
Mar 18, 2017, 7:23:16 AM3/18/17
to Materials & Welding
Dear guys,

I am dining Welding between SS to CS by use of ER309LT1-1 but can not get weld bead ripples same as carbon steel Welding Please, suggest any Welding Techniques for the same.

Kannayeram Gnanapandithan

unread,
Mar 18, 2017, 9:12:30 AM3/18/17
to materials-welding
what is the shielding gas used. weld parameters. pl correct to E309T1-1

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, Mar 18, 2017 at 2:55 PM, PARESH JADAV <paresh...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (paresh...@gmail.com) Add cleanup rule | More info

Dear guys,

I am dining Welding between SS to CS by use of ER309LT1-1 but can not get weld bead ripples same as carbon steel Welding Please, suggest any Welding Techniques for the same.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d1ae1ba1-5103-4371-9b3e-c422d998e76e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages