PQR WPQ certified

53 views
Skip to first unread message

Shaunak Upadhyay

unread,
Feb 18, 2016, 6:56:42 AM2/18/16
to Materials & Welding
Dear All,

Please clarify below points, if have reference standard also write in your reply.

1. PQR in ASME - Certified by Manufacturer
Who can certified PQR? QC manager or welding engineer?
In my company no have welding manager. So who can certify PQR.

2. WPQ in ASME - Certified by Manufacture
Who can certified?
Same question as above.

3. WPS in ASME -
WPS require approved by QC Manager or welding engineer can approve this ?

Please reply your valuable answer and if have specific ASME clause number let me know.

Thanks in advance.

Regards
Shaunak.
shanup...@gmail.com

Kannayeram Gnanapandithan

unread,
Feb 18, 2016, 7:05:36 AM2/18/16
to materials-welding
MANUFACTURER HAS TO CERTIFY AND APPROVE, WITHIN COMPANY , PERSON MAY BE FROM QUALITY, PRODUCTION OR WELDING.

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d0a84f3d-85a6-4c51-a2ec-a5ea1ae7beb5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

santo...@gmail.com

unread,
Feb 18, 2016, 7:17:55 AM2/18/16
to material...@googlegroups.com
Dear Mr Shaunak
Generally Welding Engineer is preparing the above procedure and QCM will approve the same

But as per your mail you are ASME certified company ,so please refer your company's ASME Quality Manual which is approved by ASME Authorised Inspector.

Thanks and Regards