Impact Sub-size specimen

29 views
Skip to first unread message

ABHISHEK SINGH

unread,
Jun 28, 2020, 2:14:16 AM6/28/20
to Materials & Welding
Dear Experts,

I am having query regarding impact test as per ISO EN standard.
1) Is any temperature reduction is applicable for impact sub-size specimen?
2) Any joule value relaxation for impact sub-size specimen.

Regards
Abhishek Singh

Raghul

unread,
Jun 29, 2020, 1:06:48 AM6/29/20
to material...@googlegroups.com

Hi

Temperature reduction is applicable for sub size specimen and there is no relaxation for joule value.

Sent from my iPhone

> On 28-Jun-2020, at 11:44 AM, ABHISHEK SINGH <mech....@gmail.com> wrote:
>
> Dear Experts,
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c9483c40-6376-464d-8a60-e49476993fc7o%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages