P-No. of UNS 06626

211 views
Skip to first unread message

ilham fauzi

unread,
Feb 28, 2024, 5:13:00 AMFeb 28
to Materials & Welding
Dear Experts,

What is P-No. of UNS 06626, my client say its P No.45 but that materials simillar with UNS 06625 which is its P-No.43. Please for the advice

Thanks

Mostafa DAIF

unread,
Feb 28, 2024, 5:57:15 AMFeb 28
to material...@googlegroups.com
Dear all,
The P number is P42 according to ASME Boiler & Pressure Vessel Code Section IX;

Best Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c105a43f-72c7-44b6-96e1-0e11095552a3n%40googlegroups.com.


--

Mostafa DAIF
Chef preparateur

T : 05 23 38 90 72
M : 06 61 54 12 95
TAQA MOROCCO PB 99 Sidi Bouzid - El Jadida 24 000 - Maroc
taqamorocco.ma

TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies.
  

The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments.


cyndiso yapi

unread,
Feb 28, 2024, 5:57:20 AMFeb 28
to material...@googlegroups.com
Its P-No 43 check ASME IX Table QW422 it's listed there 

--

Chiranjeevi A

unread,
Feb 28, 2024, 5:57:31 AMFeb 28
to material...@googlegroups.com
Dear Fauzi,

Please refer to the Limiting chemical composition in MTC & concerning ASME Code Case 2276 
It should be P-No. 43



--

Chiranjeevi A

unread,
Feb 28, 2024, 8:29:11 AMFeb 28
to material...@googlegroups.com
Dear all,

Please refer to the table below for the required chemical composition of UNS 06626 under case 2276, as per the ASME BPV code cases. The P-No. for material UNS 06626 is P-43.

image.png

ilham fauzi

unread,
Feb 29, 2024, 12:35:04 AMFeb 29
to material...@googlegroups.com
Dear All Experts,

Thanks all for the advice and information. I checked ASME code case 2276-1, which states that UNS 06626 can be classified as category P-No.43.
image.png
Thanks a bunch.

Best Regards,
M Ilham Fauzi Pane
Welding Engineer


You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/SpmpHXyXbjw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zYAakAwiLyp2J3AqpDMTSFAhCZXPSKUY5ZFFYy2gTh8Q%40mail.gmail.com.

Vinay

unread,
Mar 25, 2024, 5:18:18 AMMar 25
to material...@googlegroups.com
PL confirm , it is UNS N06626 . Its Ni-Cr moly steel..   P-45 is correct.