Calculation of welding parameters

49 views
Skip to first unread message

charles

unread,
May 27, 2020, 11:22:23 AM5/27/20
to Materials & Welding
Dear experts,

Pl. Provide the calculation for finding welding parameters like current and voltage if the carbon equivalent of steel is known?. Does this work good for alloy steels also?

Regards,

Charles Jacob

rems.o...@gmail.com

unread,
May 28, 2020, 11:47:23 PM5/28/20
to material...@googlegroups.com
Dear Charles,

The choice of welding parameters like current and Voltage is dependent on the choice of welding process and consumable used and not on Carbon Equivalent. Carbon equivalent is a weldability factor which gives you sense of materials conditioning prior to welding like preheat temperature and during welding and after welding for the avoidance of welding issues like cracking.

Regards
--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.