I have situation where Air Receiver Vessel made of SS 316  designed as per ASME SEC VIII DIV 1 U stamped shipped to site but not yet installed. The vessel is stored on warehouse in packed condition.

 

The Present design temperature is 70°C which need to be changed to 85°C.

 

Can you please suggest which are steps we have to take ? Any code reference for recertification ?


 

Regards

Praphulla

george....@gr.bureauveritas.com

unread,
Oct 23, 2015, 4:43:53 AM10/23/15
to Materials-Welding
Get in touch with a R stamp holder and apply for rerating/alteration

Sent from my BlackBerry 10 smartphone.
From: Praphulla Phirke
Sent: Παρασκευή, 23 Οκτωβρίου 2015 - 11:11
To: Materials-Welding
Subject: [MW:23779] Vessel Design Temperature Change

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/341D89B8-0E22-4517-AE8D-5DD65D81A0F5%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Mohd Azam

unread,
Oct 24, 2015, 1:17:34 AM10/24/15
to material...@googlegroups.com

Design only need to be verified, Nothing to do with vessel, However change in temperature is small and only in plus side. Hopefully there will be no R-Stamp.

 

Thanks & Regards,

Mohd. Azam

--

Praphulla Phirke

unread,
Oct 24, 2015, 2:01:19 AM10/24/15
to material...@googlegroups.com
Hi Mohd.Azam
Do you know some code extras which will permit us to do this modifications?


Warm Regards
Praphulla
Sent from my iPhone

Praphulla Phirke

unread,
Oct 24, 2015, 3:38:04 AM10/24/15
to material...@googlegroups.com
Dear Sir
Thanks a lot.. Do you suggest some code reference ? The manufacture demanding us the code reference .



Warm Regards
Praphulla
Sent from my iPhone

Mohd Azam

unread,
Oct 24, 2015, 3:47:05 AM10/24/15
to material...@googlegroups.com

This has to be confirm from designer end. Design verification is to be done and confirm from his end that there is no need for any change in vessel Drawing.

 

Thanks & Regards,

Mohd. Azam

george....@gr.bureauveritas.com

unread,
Oct 24, 2015, 4:14:06 AM10/24/15
to Mohd Azam
The "R" stamp is always required even the alteration us minor. The AI involvement is different

Sent from my BlackBerry 10 smartphone.
From: Mohd Azam
Sent: Σάββατο, 24 Οκτωβρίου 2015 - 08:17
Subject: Re: [MW:23787] Vessel Design Temperature Change


For more options, visit https://groups.google.com/d/optout.

george....@gr.bureauveritas.com

unread,
Oct 24, 2015, 4:27:37 AM10/24/15
to Praphulla Phirke
National Board Inspection Code part 3

Sent from my BlackBerry 10 smartphone.
From: Praphulla Phirke
Sent: Σάββατο, 24 Οκτωβρίου 2015 - 10:38
Subject: Re: [MW:23795] Vessel Design Temperature Change


For more options, visit https://groups.google.com/d/optout.

Perumal Govindan

unread,
Oct 24, 2015, 4:37:13 AM10/24/15
to material...@googlegroups.com

Hi

Please revise the design documents and get it approved by ASME AI & by Client as well.
If already applied for NBR, revise and resubmit for registration again (including the changes).

Regards
P
Govindan

george....@gr.bureauveritas.com

unread,
Oct 24, 2015, 6:45:24 AM10/24/15
to Perumal Govindan
A Code vessel can not be stamped two times with a Code stamp. In case of repair, alteration or re rating it has to be stamped with the "R" stamp‎.

Sent from my BlackBerry 10 smartphone.
From: Perumal Govindan
Sent: Σάββατο, 24 Οκτωβρίου 2015 - 11:37
Subject: Re: [MW:23800] Vessel Design Temperature Change


For more options, visit https://groups.google.com/d/optout.

pgoswami

unread,
Oct 24, 2015, 10:55:26 AM10/24/15
to material...@googlegroups.com

Hi Praphulla

The vessel should be rerated. You may use the approach as recommended by NBIC or API-510.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist

Hamilton, Ontario, Canada

pgos...@quickclic.net

pradip....@gmail.com

ca.linkedin.com/pub/pradip-goswami/5/985/299

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of george....@gr.bureauveritas.com
Sent: Saturday, October 24, 2015 6:32 AM
To: Perumal Govindan; material...@googlegroups.com
Subject: Re: [MW:23802] Vessel Design Temperature Change

 

A Code vessel can not be stamped two times with a Code stamp. In case of repair, alteration or re rating it has to be stamped with the "R" stamp.

 

Sent from my BlackBerry 10 smartphone.

From: Perumal Govindan

Sent: Σάββατο, 24 Οκτωβρίου 2015 - 11:37

Subject: Re: [MW:23800] Vessel Design Temperature Change

 

Hi

Please revise the design documents and get it approved by ASME AI & by Client as well. If already applied for NBR, revise and resubmit for registration again (including the changes).

Regards

P.Govindan