Dear experts

We have to weld 30” dia and 25 mm thickness of aluminum materials .

suggest me alternative of RT, PAUT , joints are confined area

1. Due to space RT is difficult , and for PAUT additional material not available to prepare test pieces / calibration blocks

Best Regards


vishal.n...@gmail.com

unread,
Aug 2, 2023, 11:19:41 PM8/2/23
to material...@googlegroups.com
Dear Mr. Ali,

We can support for calibration block and inspection by PAUT, as we have aluminum block available with us. 

If you require support for the same, you can write us on in...@ndtsolutions.co.in.

Regards,
Vishal Gherwada
ASNT LEVEL III -UT
ISO 9712 LEVELV III - UT & PAUT

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages