thickness on painted vessel

59 views
Skip to first unread message

Kumar

unread,
Nov 14, 2016, 10:34:32 PM11/14/16
to material...@googlegroups.com
Dear Experts,

Greetings.

Just expecting your views for the UT- thickness measurements on a
painted pressure vessel (shell thick 54 mm & head 65mm) painting
thickness -250 microns. material SA 516 Gr. 70 N.

The construction phase is going on but few vessels are painted but
baseline thickness measures to be taken. Awaiting valuable feedbacks
pl.

Thanks in advance,

Kumar.

Nitin Shetty

unread,
Nov 15, 2016, 9:35:14 PM11/15/16
to material...@googlegroups.com
Dear Kumar,

If the vessel is not coated from inside the thickness can be measured from inside too. For small bore nozzles also you get special probe which can be used to check the thickness of Pipe wall. However coming back to your question whether UT can be performed after painting my answer is NO using a conventional UT machine with zero degree probe. How ever you can use thickness gauging machine to check the wall and there are machines which can be used where the DFT is upto 2000 microns especially used for marine applications.

Regards,

Nitin Shetty.

Regards,

Nitin Shetty


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp_UbmLrh-owzxWBk7cEm%2Bi3Yr0BYRMYge7Jn8b1HFN2Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Prasad Rode

unread,
Nov 15, 2016, 9:35:15 PM11/15/16
to Materials & Welding
Whts u r question is? Pls clarify.
To perform the Ut , u have to remove the paint.

Regards
Prasad Rode

ECHARU

unread,
Nov 15, 2016, 10:17:19 PM11/15/16
to material...@googlegroups.com
Dear experts,
Please check with your third party ndt UT technical, there are  some gauges available to measure to coating and steel thickness without removing coating. Yesterday, we conducted at this method.
To measure the thickness only.
Thankyou

From: Prasad Rode
Sent: ‎16-‎11-‎2016 05:35
To: Materials & Welding
Subject: [MW:25707] thickness on painted vessel

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f105f84b-66bb-40de-af09-9548f40acd8c%40googlegroups.com.

pgoswami

unread,
Nov 15, 2016, 10:31:54 PM11/15/16
to material...@googlegroups.com, sk79...@gmail.com

 

Hi Kumar,

 

Please take a look at the following article and suggested techniques. Olympus is a global company with many resources. A discussion may be of help.

 

Thanks.

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist ,

Ontario,Canada.

ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 

http://www.olympus-ims.com/en/applications/measuring-metal-thickness-paint/

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

To post to this group, send email to material...@googlegroups.com.

Measuring Metal Thickness Through Paint.pdf

Luciano Lucas

unread,
Nov 16, 2016, 7:23:27 AM11/16/16
to material...@googlegroups.com
Prasard,
No you don't!
There are UT equipment's allowed take measurements...
without take paint..

regards,

Luciano Lucas




-----Mensagem original-----
De: material...@googlegroups.com [mailto:material...@googlegroups.com] Em nome de Prasad Rode
Enviada: terça-feira, 15 de Novembro de 2016 17:34
Para: Materials & Welding
Assunto: [MW:25707] thickness on painted vessel
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f105f84b-66bb-40de-af09-9548f40acd8c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

________________________________

O conteúdo desta mensagem de correio eletrónico e seus anexos é confidencial e de uso reservado.
Se não é o destinatário, não a guarde, não a reenvie a terceiros, nem faça qualquer uso da informação nela contida. Por favor, apague-a e informe de imediato o remetente. A Internet não garante a confidencialidade e a entrega correta de mensagens de correio eletrónico. A Galp não aceita responsabilidade por danos causados pela receção incorreta desta mensagem.
Apesar de esta mensagem ter sido verificada pelo nosso sistema de antivírus, não podemos garantir que não contenha vírus informáticos e não aceitamos qualquer responsabilidade por danos causados por vírus que possam estar contidos nesta mensagem.
Para informações sobre a Galp visite o nosso website em http://www.galp.com.

This e-mail and related attachments contain confidential and legally privileged information.
If you are not the intended recipient you must not keep it in your records or forward it to any third parties, nor use the information contained in it. Please delete it and notify by return Email. Internet email does not guarantee the confidentiality or the proper receipt of messages sent. Galp declines any liability for damages caused by improper receipt of this message.
Our own virus checking system has swept this e-mail and its attachments. However, we cannot guarantee that it is vírus-free and cannot take responsibility for any virus which may be present.
For further information about Galp please visit our website at http://www.galp.com.

José Juan Jiménez Alejandro

unread,
Nov 16, 2016, 10:08:18 PM11/16/16
to material...@googlegroups.com
I do not understand your question well, but according to the comments, you want to measure the wall thickness of the vessel already painted, my answer is that IF you can measure the thickness of the wall with Ultrasound measuring equipment thickness, but you need to have The function to discriminate paint, generally the modern equipments bring this function, you do not have to remove or remove the painting in any moment and can be inspected from the outside than if painted. I hope I've helped.
Regards!.


For more options, visit https://groups.google.com/d/optout.



--

Ing. José Juan Jiménez Alejandro

Cel. 812 103 1155

Skype: jjjimeneza

Reply all
Reply to author
Forward
0 new messages