Dear all ,

Can some one Tell me that why are we take pneumatic test of RF pad of
pressure vessels nozzle???

TDK YOKESH

unread,
Apr 1, 2015, 12:09:29 AM4/1/15
to material...@googlegroups.com
Warm Greetings ,

We don't call it Pneumatic Test . We call it Leak test which is done to check weld integrity at the RF pad and nozzle by applying pressure through the vent hole and check the weldment with Snoop solution . 
 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V_5nq7hurgbta5XPCe3jx2cs1d3DP6GvUiAmLXD200jVQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--

Best regards,

TDK YOKESH

QC INSPECTOR ( PIPING AND WELDING )

QUALITY CONTROL DEPARTMENT

https://encrypted-tbn0.gstatic.com/images?q=tbn:ANd9GcQ7lSlmn1ExpyOpkX2RaZW-T5JttIFRfJMtPb23EzPZOQxDBU2w8PO-rDQ

Plot D1, Lumut Port Industrial Park,

Kg. Acheh, Mukim of Lumut,

Daerah Manjung, 32000 Sitiawan,

Perak Darul Ridzuan,

Malaysia

Tel No. : +601126527600

Email: tdk...@gmail.com

Hareesh K V

unread,
Apr 1, 2015, 12:40:34 AM4/1/15
to materials-welding

Dear Mr.Rahul,

The pneumatic test of RF pad is done to ensure that no leak is there inside the area of RF pad. That is, particularly in the nozzle to vessel joint and RF pad to nozzle joint. The integrity of  fillet weld of RF pad to vessel is also ensured by this process ( It is ensured that no leak is  there inside the RF pad, due to welding of the RF pad to vessel joint)

In the pressure test of vessel, leak inside the RF pad may not get detected, if the % of leak is very less.

Regards
Hareesh K V

On Apr 1, 2015 9:39 AM, "TDK YOKESH" <tdk...@gmail.com> wrote:
>
> Warm Greetings ,
>
> We don't call it Pneumatic Test . We call it Leak test which is done to check weld integrity at the RF pad and nozzle by applying pressure through the vent hole and check the weldment with Snoop solution . 
>  
>
> On Tue, Mar 31, 2015 at 11:54 PM, Rahul Chaudhari <navy...@gmail.com> wrote:
>>
>> Dear all ,
>>
>> Can some one Tell me that why are we take pneumatic test of RF pad of
>> pressure vessels nozzle???
>>
>> --
>> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
>> To post to this group, send email to material...@googlegroups.com.
>> Visit this group at http://groups.google.com/group/materials-welding.
>> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V_5nq7hurgbta5XPCe3jx2cs1d3DP6GvUiAmLXD200jVQ%40mail.gmail.com.
>> For more options, visit https://groups.google.com/d/optout.
>
>
>
>
> --
>
> Best regards,
>
> TDK YOKESH
>
> QC INSPECTOR ( PIPING AND WELDING )
>
> QUALITY CONTROL DEPARTMENT
>

> Plot D1, Lumut Port Industrial Park,
>
> Kg. Acheh, Mukim of Lumut,
>
> Daerah Manjung, 32000 Sitiawan,
>
> Perak Darul Ridzuan,
>
> Malaysia
>
> Tel No. : +601126527600
>
> Email: tdk...@gmail.com
>

> --
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> To post to this group, send email to material...@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.

> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuraZ0u8OZvNyFM9Cuf5mrMEA7Qru4WbZsqK2ajkVkMfyQ%40mail.gmail.com.

gprak...@gmail.com

unread,
Apr 1, 2015, 12:57:27 AM4/1/15
to materials-welding
Yes. It is called air leak test. Normally the pr is little more than 1 bar and checked by soap solution or any other method

Rgds
 Prakash. G. 
ASME AIS
Independent Consultant. ASME/ISO/PED
From: Hareesh K V
Sent: Wednesday, 1 April 2015 08:40
To: materials-welding
Subject: Re: [MW:23028] pneumatic test of RF pad of nozzle