Welding position here is as per ISO 15614-1 Not AWS D1.1 as i said before and clearly mentioned in WPS and subject title
as per ISO 15164-1
This means only PG and H-LO45 need to be separately qualified , and if qualified for any position all other position will be qualified except PG and HI-LO45
My case here in over head welding (5G See below Sketch ) so PG will cover all position expect HI-LO45
For Current and voltage this values are taken already from actual WPS/PQR but according to AWS D1.1 as i told you i need only to convert it to BS EN
this Preliminary WPS as you know actual values will be recorded and written during running of final PQR
Trade name and brand is not mandatory variable here too
Hope it is clear now
Regards,
H.A